Related Material — 65.7% match
based on chemical composition and mechanical property overlap.
AISI 1010 and BS 970 (Part 1) 045M10 (BS 970 (Part 1):1991) are both steel grades.
Both fall under the Carbon Steel category.
AISI 1010 is typically used for tubing, pipe, sheet, structural shapes, wire, while BS 970 (Part 1) 045M10 is commonly used for case hardening steel (section four).
AISI 1010 is defined under AISI, originating from United States, while BS 970 (Part 1) 045M10 is defined under British Standards (BS), originating from United Kingdom.
As per chemical composition, AISI 1010 vs BS 970 (Part 1) 045M10 is a 98.6% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a related material overall at 65.7%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
AISI 1010
BS 970 (Part 1) 045M10
Tensile Strength
340–470 MPa
430 MPa min
Elongation
≥26%
18 % min
Hardness
≤137 HB
Not specified
Condition
Not specified
Case hardened, 19 mm test bar
Typical Applications
AISI 1010
Tubing, pipe, sheet, structural shapes, wire
BS 970 (Part 1) 045M10
Case hardening steel (section four)
Key Differences
AISI 1010 specifies S, P which are not specified for BS 970 (Part 1) 045M10.
Can AISI 1010 Be Substituted With BS 970 (Part 1) 045M10?
AISI 1010 and BS 970 (Part 1) 045M10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between AISI 1010 and BS 970 (Part 1) 045M10?
AISI 1010 specifies S, P which are not specified for BS 970 (Part 1) 045M10.
Can AISI 1010 be substituted with BS 970 (Part 1) 045M10?
AISI 1010 and BS 970 (Part 1) 045M10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.