Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Mn
S
P
0.50–0.60
0.60–0.90
≤0.050
≤0.030
Mechanical Properties
Condition
Hot Rolled
Tensile Strength
700-750 MPa
Yield Strength
380-450 MPa
Elongation
12-16%
Hardness
197-220 HB
Typical Available Sizes
Round Bar
10mm–150mm dia
Wire Rod Coil
5.5mm–25mm dia
Flat Bar
16×5mm–150×30mm