ASTM A959 SS316 vs IS 1570 (Part 7) 12Cr12MoH

Related Material — 59.9% match based on chemical composition and mechanical property overlap.

ASTM A959 SS316 (ASTM A959:2011) and IS 1570 (Part 7) 12Cr12MoH (IS 1570 (Part 7):1992) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 SS316 is typically used for marine, chemical, pharmaceutical, food processing equipment, while IS 1570 (Part 7) 12Cr12MoH is commonly used for boilers, pressure vessels, steam turbines, steam and water piping and other power plant equipment working at elevated temperature. ASTM A959 SS316 is defined under ASTM International, originating from United States, while IS 1570 (Part 7) 12Cr12MoH is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, ASTM A959 SS316 vs IS 1570 (Part 7) 12Cr12MoH is a 59.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 59.9%.

Frequently Compared With ASTM A959 SS316:
EN 10088-1 1.4401 EN 10088-1 1.4006 EN 10088-1 1.4845 EN 10088-1 1.4301 ASTM A959 .- ASTM A959 16-8-2H GOST 5632 06Kh23N28 GOST 5632 08X18H10 GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
59.9%
MECHANICAL MATCH
No shared data
OVERALL
59.9%
Specifications
Property ASTM A959 SS316 IS 1570 (Part 7) 12Cr12MoH
Standard ASTM A959:2011 IS 1570 (Part 7):1992
Category Stainless Steel Stainless Steel
C (%) <=0.08 0.08-0.16
Cr (%) 16.0-18.0 11.5-13.00
Mn (%) <=2.00 0.40-1.00
Mo (%) 2.00-3.00 0.40-0.80
Ni (%) 10.0-14.0 <=1.0
P (%) <=0.045 <=0.040
S (%) <=0.030 <=0.035
Si (%) <=1.00 <=0.60
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A959 SS316 IS 1570 (Part 7) 12Cr12MoH
Tensile Strength Not specified 680-880 MPa
Yield Strength Not specified >=490 MPa (0.2 % proof stress)
Elongation Not specified >=20%
Condition Not specified Bars, forgings, Q+T, thickness up to 75 (first row of Table 3)
Typical Applications
ASTM A959 SS316
Marine, chemical, pharmaceutical, food processing equipment
IS 1570 (Part 7) 12Cr12MoH
Boilers, pressure vessels, steam turbines, steam and water piping and other power plant equipment working at elevated temperature
Can ASTM A959 SS316 Be Substituted With IS 1570 (Part 7) 12Cr12MoH?
ASTM A959 SS316 and IS 1570 (Part 7) 12Cr12MoH share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
ASTM A959 SS316
Sheet → (24 listings)
Thickness: 2–6 mm (0.08–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–4000 mm (98.43–157.48 in)
Plate → (6 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2600–4200 mm (102.36–165.35 in)
Round Bar → (3 listings)
Diameter: 40–40 mm (1.57–1.57 in)
Length: 2500–4200 mm (98.43–165.35 in)
IS 1570 (Part 7) 12Cr12MoH
No active listings currently.
On M-EX Right Now
ASTM A959 SS316
33 active listings and RFQs →
IS 1570 (Part 7) 12Cr12MoH
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 SS316 and IS 1570 (Part 7) 12Cr12MoH?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A959 SS316 be substituted with IS 1570 (Part 7) 12Cr12MoH?
ASTM A959 SS316 and IS 1570 (Part 7) 12Cr12MoH share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.