ASTM A240/A240M N08800 vs ASTM A276/A276M N08800

Strong Match — 88.9% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M N08800 (ASTM A240/A240M:2025) and ASTM A276/A276M N08800 (ASTM A276/A276M:2017) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M N08800 is typically used for pressure vessels and general applications (plate, sheet and strip), while ASTM A276/A276M N08800 is commonly used for stainless steel bars and shapes (hot-finished or cold-finished). ASTM A240/A240M N08800 is defined under ASTM International, originating from United States, while ASTM A276/A276M N08800 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A240/A240M N08800 vs ASTM A276/A276M N08800 is a 100% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a strong match overall at 88.9%.

Frequently Compared With ASTM A240/A240M N08800:
EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
66.7%
OVERALL
88.9%
Specifications
Property ASTM A240/A240M N08800 ASTM A276/A276M N08800
Standard ASTM A240/A240M:2025 ASTM A276/A276M:2017
Category Stainless Steel Stainless Steel
C (%) <=0.10 <=0.10
Mn (%) <=1.50 <=1.50
P (%) <=0.045 <=0.045
S (%) <=0.015 <=0.015
Si (%) <=1.00 <=1.00
Cr (%) 19.0-23.0 19.0-23.0
Ni (%) 30.0-35.0 30.0-35.0
Cu (%) <=0.75 <=0.75
Fe (%) >=39.5 >=39.5
Al (%) 0.15-0.60 0.15-0.60
Ti (%) 0.15-0.60 0.15-0.60
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M N08800 ASTM A276/A276M N08800
Tensile Strength >=520 MPa >=515 MPa
Yield Strength >=205 MPa >=205 MPa
Elongation >=30% >=30%
Condition Plate, sheet and strip; yield by 0.2 percent offset Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed)
Hardness Not specified <=192 HB
Typical Applications
ASTM A240/A240M N08800
Pressure vessels and general applications (plate, sheet and strip)
ASTM A276/A276M N08800
Stainless steel bars and shapes (hot-finished or cold-finished)
Can ASTM A240/A240M N08800 Be Substituted With ASTM A276/A276M N08800?
ASTM A240/A240M N08800 and ASTM A276/A276M N08800 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M N08800 is often considered as a substitute for ASTM A240/A240M N08800 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M N08800
0 active listings and RFQs →
ASTM A276/A276M N08800
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M N08800 and ASTM A276/A276M N08800?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A240/A240M N08800 be substituted with ASTM A276/A276M N08800?
ASTM A240/A240M N08800 and ASTM A276/A276M N08800 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M N08800 is often considered as a substitute for ASTM A240/A240M N08800 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.