ASTM A240/A240M N08811 vs EN 10088-1 X10NiCrAlTi32-21

Strong Match — 86.3% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M N08811 (ASTM A240/A240M:2025) and EN 10088-1 X10NiCrAlTi32-21 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M N08811 is defined under ASTM International, originating from United States, while EN 10088-1 X10NiCrAlTi32-21 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A240/A240M N08811 vs EN 10088-1 X10NiCrAlTi32-21 is a 86.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 86.3%.

Frequently Compared With ASTM A240/A240M N08811:
EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
86.3%
MECHANICAL MATCH
No shared data
OVERALL
86.3%
Specifications
Property ASTM A240/A240M N08811 EN 10088-1 X10NiCrAlTi32-21
Standard ASTM A240/A240M:2025 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.06-0.10 <=0.12
Mn (%) <=1.50 <=2.00
P (%) <=0.040 <=0.030
S (%) <=0.015 <=0.015
Si (%) <=1.00 <=1.00
Cr (%) 19.0-23.0 19.0-23.0
Ni (%) 30.0-35.0 30.0-34.0
Cu (%) <=0.75 Not specified
Fe (%) >=39.5 Not specified
Ti (%) 0.25-0.60 0.15-0.60
Al (%) 0.25-0.60 0.15-0.60
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M N08811 EN 10088-1 X10NiCrAlTi32-21
Tensile Strength >=450 MPa Not specified
Yield Strength >=170 MPa Not specified
Elongation >=30% Not specified
Condition Plate, sheet and strip; yield by 0.2 percent offset Not specified
Typical Applications
ASTM A240/A240M N08811
Pressure vessels and general applications (plate, sheet and strip)
EN 10088-1 X10NiCrAlTi32-21
Not documented
Key Differences
Can ASTM A240/A240M N08811 Be Substituted With EN 10088-1 X10NiCrAlTi32-21?
ASTM A240/A240M N08811 and EN 10088-1 X10NiCrAlTi32-21 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X10NiCrAlTi32-21 is often considered as a substitute for ASTM A240/A240M N08811 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M N08811
0 active listings and RFQs →
EN 10088-1 X10NiCrAlTi32-21
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M N08811 and EN 10088-1 X10NiCrAlTi32-21?
ASTM A240/A240M N08811 specifies Cu, Fe which are not specified for EN 10088-1 X10NiCrAlTi32-21.
Can ASTM A240/A240M N08811 be substituted with EN 10088-1 X10NiCrAlTi32-21?
ASTM A240/A240M N08811 and EN 10088-1 X10NiCrAlTi32-21 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X10NiCrAlTi32-21 is often considered as a substitute for ASTM A240/A240M N08811 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.