ASTM A240/A240M S30451 vs EN 10088-1 X5CrNiN19-9

Strong Match — 90% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S30451 (ASTM A240/A240M:2025) and EN 10088-1 X5CrNiN19-9 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S30451 is defined under ASTM International, originating from United States, while EN 10088-1 X5CrNiN19-9 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A240/A240M S30451 vs EN 10088-1 X5CrNiN19-9 is a 90% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 90%.

Frequently Compared With ASTM A240/A240M S30451:
GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12Ni2Mo EN 10088-1 1.4006 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr13H ASTM A959 .- GOST 5632 06Kh23N28 GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
90%
MECHANICAL MATCH
No shared data
OVERALL
90%
Specifications
Property ASTM A240/A240M S30451 EN 10088-1 X5CrNiN19-9
Standard ASTM A240/A240M:2025 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.06
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.015
Si (%) <=0.75 <=1.00
Cr (%) 18.0-20.0 18.0-20.0
Ni (%) 8.0-10.5 8.0-11.0
N (%) 0.10-0.16 0.12-0.22
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S30451 EN 10088-1 X5CrNiN19-9
Tensile Strength >=550 MPa Not specified
Yield Strength >=240 MPa Not specified
Elongation >=30% Not specified
Hardness <=217 HB Not specified
Condition Plate, sheet and strip; yield by 0.2 percent offset Not specified
Typical Applications
ASTM A240/A240M S30451
Pressure vessels and general applications (plate, sheet and strip)
EN 10088-1 X5CrNiN19-9
Not documented
Can ASTM A240/A240M S30451 Be Substituted With EN 10088-1 X5CrNiN19-9?
ASTM A240/A240M S30451 and EN 10088-1 X5CrNiN19-9 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X5CrNiN19-9 is often considered as a substitute for ASTM A240/A240M S30451 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M S30451
0 active listings and RFQs →
EN 10088-1 X5CrNiN19-9
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S30451 and EN 10088-1 X5CrNiN19-9?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A240/A240M S30451 be substituted with EN 10088-1 X5CrNiN19-9?
ASTM A240/A240M S30451 and EN 10088-1 X5CrNiN19-9 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X5CrNiN19-9 is often considered as a substitute for ASTM A240/A240M S30451 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.