ASTM A240/A240M S31041 vs ASTM A240/A240M S31040

Strong Match — 94.8% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S31041 (ASTM A240/A240M:2025) and ASTM A240/A240M S31040 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S31041 is typically used for pressure vessels and general applications (plate, sheet and strip), while ASTM A240/A240M S31040 is commonly used for pressure vessels and general applications (plate, sheet and strip). ASTM A240/A240M S31041 is defined under ASTM International, originating from United States, while ASTM A240/A240M S31040 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A240/A240M S31041 vs ASTM A240/A240M S31040 is a 92.2% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 94.8%.

Frequently Compared With ASTM A240/A240M S31041:
GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH GB/T 3280 06Cr19Ni10 EN 10088-1 1.4301 EN 10088-1 1.4401 ASTM A959 .- EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
92.2%
MECHANICAL MATCH
100%
OVERALL
94.8%
Specifications
Property ASTM A240/A240M S31041 ASTM A240/A240M S31040
Standard ASTM A240/A240M:2025 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) 0.04-0.10 <=0.08
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=0.75 <=1.50
Cr (%) 24.0-26.0 24.0-26.0
Ni (%) 19.0-22.0 19.0-22.0
Nb (%) <=1.10 <=1.10
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S31041 ASTM A240/A240M S31040
Tensile Strength >=515 MPa >=515 MPa
Yield Strength >=205 MPa >=205 MPa
Elongation >=40% >=40%
Hardness <=217 HB <=217 HB
Condition Plate, sheet and strip; yield by 0.2 percent offset Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
ASTM A240/A240M S31041
Pressure vessels and general applications (plate, sheet and strip)
ASTM A240/A240M S31040
Pressure vessels and general applications (plate, sheet and strip)
Can ASTM A240/A240M S31041 Be Substituted With ASTM A240/A240M S31040?
ASTM A240/A240M S31041 and ASTM A240/A240M S31040 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S31040 is often considered as a substitute for ASTM A240/A240M S31041 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M S31041
0 active listings and RFQs →
ASTM A240/A240M S31040
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S31041 and ASTM A240/A240M S31040?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A240/A240M S31041 be substituted with ASTM A240/A240M S31040?
ASTM A240/A240M S31041 and ASTM A240/A240M S31040 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S31040 is often considered as a substitute for ASTM A240/A240M S31041 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.