ASTM A240/A240M S31730 vs ASTM A276/A276M S31730

Strong Match — 100% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S31730 (ASTM A240/A240M:2025) and ASTM A276/A276M S31730 (ASTM A276/A276M:2017) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S31730 is typically used for pressure vessels and general applications (plate, sheet and strip), while ASTM A276/A276M S31730 is commonly used for stainless steel bars and shapes (hot-finished or cold-finished). ASTM A240/A240M S31730 is defined under ASTM International, originating from United States, while ASTM A276/A276M S31730 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A240/A240M S31730 vs ASTM A276/A276M S31730 is a 100% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 100%.

Frequently Compared With ASTM A240/A240M S31730:
GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
100%
OVERALL
100%
Specifications
Property ASTM A240/A240M S31730 ASTM A276/A276M S31730
Standard ASTM A240/A240M:2025 ASTM A276/A276M:2017
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Mn (%) <=2.00 <=2.00
P (%) <=0.040 <=0.040
S (%) <=0.010 <=0.010
Si (%) <=1.00 <=1.00
Cr (%) 17.0-19.0 17.0-19.0
Ni (%) 15.0-16.5 15.0-16.5
Mo (%) 3.0-4.0 3.0-4.0
N (%) <=0.045 <=0.045
Cu (%) 4.0-5.0 4.0-5.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S31730 ASTM A276/A276M S31730
Tensile Strength >=480 MPa >=480 MPa
Yield Strength >=175 MPa >=175 MPa
Elongation >=35% >=35%
Hardness <=90 HRBW <=90 HRB
Condition Plate, sheet and strip; yield by 0.2 percent offset Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed)
Typical Applications
ASTM A240/A240M S31730
Pressure vessels and general applications (plate, sheet and strip)
ASTM A276/A276M S31730
Stainless steel bars and shapes (hot-finished or cold-finished)
Can ASTM A240/A240M S31730 Be Substituted With ASTM A276/A276M S31730?
ASTM A240/A240M S31730 and ASTM A276/A276M S31730 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S31730 is often considered as a substitute for ASTM A240/A240M S31730 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M S31730
0 active listings and RFQs →
ASTM A276/A276M S31730
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S31730 and ASTM A276/A276M S31730?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A240/A240M S31730 be substituted with ASTM A276/A276M S31730?
ASTM A240/A240M S31730 and ASTM A276/A276M S31730 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S31730 is often considered as a substitute for ASTM A240/A240M S31730 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.