ASTM A240/A240M S33426 vs EN 10088-1 X2CrTi21

Related Material — 69.9% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S33426 (ASTM A240/A240M:2025) and EN 10088-1 X2CrTi21 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S33426 is defined under ASTM International, originating from United States, while EN 10088-1 X2CrTi21 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A240/A240M S33426 vs EN 10088-1 X2CrTi21 is a 71.6% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 69.9%.

Frequently Compared With ASTM A240/A240M S33426:
GOST 5632 06Kh23N28 ASTM A959 29-4C GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
71.6%
MECHANICAL MATCH
No shared data
OVERALL
69.9%
Specifications
Property ASTM A240/A240M S33426 EN 10088-1 X2CrTi21
Standard ASTM A240/A240M:2025 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Mn (%) <=1.00 <=1.00
P (%) <=0.030 <=0.050
S (%) <=0.015 <=0.050
Si (%) 0.80-1.50 <=1.00
Cr (%) 19.5-22.0 19.0-22.0
Ni (%) 19.0-21.0 <=0.50
Mo (%) 1.80-2.20 <=0.50
Cu (%) Not specified <=0.50
Al (%) Not specified <=0.05
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S33426 EN 10088-1 X2CrTi21
Tensile Strength >=515 MPa Not specified
Yield Strength >=205 MPa Not specified
Elongation >=30% Not specified
Hardness <=217 HB Not specified
Condition t <= 0.12 in. [3 mm] (first condition printed); yield by 0.2 percent offset Not specified
Typical Applications
ASTM A240/A240M S33426
Pressure vessels and general applications (plate, sheet and strip)
EN 10088-1 X2CrTi21
Not documented
Key Differences
Can ASTM A240/A240M S33426 Be Substituted With EN 10088-1 X2CrTi21?
ASTM A240/A240M S33426 and EN 10088-1 X2CrTi21 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
ASTM A240/A240M S33426
0 active listings and RFQs →
EN 10088-1 X2CrTi21
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S33426 and EN 10088-1 X2CrTi21?
EN 10088-1 X2CrTi21 specifies Cu, Al which are not specified for ASTM A240/A240M S33426.
Can ASTM A240/A240M S33426 be substituted with EN 10088-1 X2CrTi21?
ASTM A240/A240M S33426 and EN 10088-1 X2CrTi21 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.