ASTM A240/A240M S44800 vs EN 10088-1 1.4845

Minimal Match — 34.2% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S44800 (ASTM A240/A240M:2025) and EN 10088-1 1.4845 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S44800 is typically used for pressure vessels and general applications (plate, sheet and strip), while EN 10088-1 1.4845 is commonly used for furnace parts, heat exchangers, kiln components. ASTM A240/A240M S44800 is defined under ASTM International, originating from United States, while EN 10088-1 1.4845 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A240/A240M S44800 vs EN 10088-1 1.4845 is a 51.3% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 34.2%.

Frequently Compared With ASTM A240/A240M S44800:
ASTM A959 29-4 ASTM A959 29-4-2 ASTM A959 29-4C EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28
Match Breakdown
CHEMISTRY MATCH
51.3%
MECHANICAL MATCH
0%
OVERALL
34.2%
Specifications
Property ASTM A240/A240M S44800 EN 10088-1 1.4845
Standard ASTM A240/A240M:2025 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.010 ≤0.10
Mn (%) <=0.30 ≤2.00
P (%) <=0.025 Not specified
S (%) <=0.020 Not specified
Si (%) <=0.20 ≤1.50
Cr (%) 28.0-30.0 24.0–26.0
Ni (%) 2.00-2.50 19.0–22.0
Mo (%) 3.5-4.2 Not specified
N (%) <=0.020 Not specified
Cu (%) <=0.15 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S44800 EN 10088-1 1.4845
Tensile Strength >=550 MPa ≥515 MPa
Yield Strength >=415 MPa ≥205 MPa
Elongation >=20% ≥40%
Hardness <=223 HB Not specified
Condition Plate, sheet and strip; yield by 0.2 percent offset Not specified
Max Service Temp Not specified 1100°C continuous
Typical Applications
ASTM A240/A240M S44800
Pressure vessels and general applications (plate, sheet and strip)
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
Key Differences
Can ASTM A240/A240M S44800 Be Substituted With EN 10088-1 1.4845?
ASTM A240/A240M S44800 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
ASTM A240/A240M S44800
No active listings currently.
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
On M-EX Right Now
ASTM A240/A240M S44800
0 active listings and RFQs →
EN 10088-1 1.4845
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S44800 and EN 10088-1 1.4845?
ASTM A240/A240M S44800 specifies P, S, Mo, N which are not specified for EN 10088-1 1.4845.
Can ASTM A240/A240M S44800 be substituted with EN 10088-1 1.4845?
ASTM A240/A240M S44800 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.