ASTM A276/A276M N08904 vs JIS G4305 SUS890L

Strong Match — 86.8% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M N08904 (ASTM A276/A276M:2017) and JIS G4305 SUS890L (JIS G4305:2012) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M N08904 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while JIS G4305 SUS890L is commonly used for cold-rolled stainless steel plates, sheet and strip. ASTM A276/A276M N08904 is defined under ASTM International, originating from United States, while JIS G4305 SUS890L is defined under Japanese Industrial Standards (JIS), originating from Japan.

As per chemical composition, ASTM A276/A276M N08904 vs JIS G4305 SUS890L is a 96.8% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a strong match overall at 86.8%.

Frequently Compared With ASTM A276/A276M N08904:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
96.8%
MECHANICAL MATCH
66.7%
OVERALL
86.8%
Specifications
Property ASTM A276/A276M N08904 JIS G4305 SUS890L
Standard ASTM A276/A276M:2017 JIS G4305:2012
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.035 <=0.030
Si (%) <=1.00 <=1.00
Cr (%) 19.0-23.0 19.00-23.00
Ni (%) 23.0-28.0 23.00-28.00
Mo (%) 4.0-5.0 4.00-5.00
N (%) <=0.10 Not specified
Cu (%) 1.0-2.0 1.00-2.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M N08904 JIS G4305 SUS890L
Tensile Strength >=490 MPa >=490 MPa
Yield Strength >=220 MPa >=215 MPa
Elongation >=35% >=35%
Condition Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed) Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser
Hardness Not specified <=187 HB
Typical Applications
ASTM A276/A276M N08904
Stainless steel bars and shapes (hot-finished or cold-finished)
JIS G4305 SUS890L
Cold-rolled stainless steel plates, sheet and strip
Key Differences
Can ASTM A276/A276M N08904 Be Substituted With JIS G4305 SUS890L?
ASTM A276/A276M N08904 and JIS G4305 SUS890L overlap closely enough on chemistry and mechanical properties that JIS G4305 SUS890L is often considered as a substitute for ASTM A276/A276M N08904 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A276/A276M N08904
0 active listings and RFQs →
JIS G4305 SUS890L
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M N08904 and JIS G4305 SUS890L?
ASTM A276/A276M N08904 specifies N which is not specified for JIS G4305 SUS890L.
Can ASTM A276/A276M N08904 be substituted with JIS G4305 SUS890L?
ASTM A276/A276M N08904 and JIS G4305 SUS890L overlap closely enough on chemistry and mechanical properties that JIS G4305 SUS890L is often considered as a substitute for ASTM A276/A276M N08904 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.