ASTM A276/A276M N08925 vs ASTM A240/A240M N08926

Close Alternative — 71% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M N08925 (ASTM A276/A276M:2017) and ASTM A240/A240M N08926 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M N08925 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while ASTM A240/A240M N08926 is commonly used for pressure vessels and general applications (plate, sheet and strip). ASTM A276/A276M N08925 is defined under ASTM International, originating from United States, while ASTM A240/A240M N08926 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A276/A276M N08925 vs ASTM A240/A240M N08926 is a 89.9% match. As per mechanical properties, the match is 33.3%. Combined, this makes them a close alternative overall at 71%.

Frequently Compared With ASTM A276/A276M N08925:
GOST 5632 06Kh23N28 ASTM A959 .- GOST 5632 08X18H10 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoVH GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4301 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
89.9%
MECHANICAL MATCH
33.3%
OVERALL
71%
Specifications
Property ASTM A276/A276M N08925 ASTM A240/A240M N08926
Standard ASTM A276/A276M:2017 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Mn (%) <=1.00 <=2.00
P (%) <=0.045 <=0.030
S (%) <=0.030 <=0.010
Si (%) <=0.50 <=0.50
Cr (%) 19.0-21.0 19.0-21.0
Ni (%) 24.0-26.0 24.0-26.0
Mo (%) 6.0-7.0 6.00-7.00
N (%) 0.10-0.20 0.15-0.25
Cu (%) 0.80-1.50 0.50-1.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M N08925 ASTM A240/A240M N08926
Tensile Strength >=600 MPa >=650 MPa
Yield Strength >=295 MPa >=295 MPa
Elongation >=40% >=35%
Hardness <=217 HB Not specified
Condition Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed) Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
ASTM A276/A276M N08925
Stainless steel bars and shapes (hot-finished or cold-finished)
ASTM A240/A240M N08926
Pressure vessels and general applications (plate, sheet and strip)
Can ASTM A276/A276M N08925 Be Substituted With ASTM A240/A240M N08926?
ASTM A276/A276M N08925 and ASTM A240/A240M N08926 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
ASTM A276/A276M N08925
0 active listings and RFQs →
ASTM A240/A240M N08926
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M N08925 and ASTM A240/A240M N08926?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M N08925 be substituted with ASTM A240/A240M N08926?
ASTM A276/A276M N08925 and ASTM A240/A240M N08926 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.