ASTM A276/A276M S30900 vs ASTM A959 309Cb

Strong Match — 92.9% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M S30900 (ASTM A276/A276M:2017) and ASTM A959 309Cb (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M S30900 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while ASTM A959 309Cb is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1). ASTM A276/A276M S30900 is defined under ASTM International, originating from United States, while ASTM A959 309Cb is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A276/A276M S30900 vs ASTM A959 309Cb is a 92.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 92.9%.

Frequently Compared With ASTM A276/A276M S30900:
EN 10088-1 1.4301 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
92.9%
MECHANICAL MATCH
No shared data
OVERALL
92.9%
Specifications
Property ASTM A276/A276M S30900 ASTM A959 309Cb
Standard ASTM A276/A276M:2017 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.20 <=0.08
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Cr (%) 22.0-24.0 22.0-24.0
Ni (%) 12.0-15.0 12.0-16.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M S30900 ASTM A959 309Cb
Tensile Strength >=515 MPa Not specified
Yield Strength >=205 MPa Not specified
Elongation >=40% Not specified
Condition Condition A (Annealed), hot-finished, all sizes (first row printed) Not specified
Typical Applications
ASTM A276/A276M S30900
Stainless steel bars and shapes (hot-finished or cold-finished)
ASTM A959 309Cb
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Can ASTM A276/A276M S30900 Be Substituted With ASTM A959 309Cb?
ASTM A276/A276M S30900 and ASTM A959 309Cb overlap closely enough on chemistry and mechanical properties that ASTM A959 309Cb is often considered as a substitute for ASTM A276/A276M S30900 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A276/A276M S30900
0 active listings and RFQs →
ASTM A959 309Cb
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M S30900 and ASTM A959 309Cb?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M S30900 be substituted with ASTM A959 309Cb?
ASTM A276/A276M S30900 and ASTM A959 309Cb overlap closely enough on chemistry and mechanical properties that ASTM A959 309Cb is often considered as a substitute for ASTM A276/A276M S30900 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.