ASTM A276/A276M S31008 vs GB/T 3280 06Cr19Ni10

Minimal Match — 54.3% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M S31008 (ASTM A276/A276M:2017) and GB/T 3280 06Cr19Ni10 (GB/T 3280-2015) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M S31008 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while GB/T 3280 06Cr19Ni10 is commonly used for used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.. ASTM A276/A276M S31008 is defined under ASTM International, originating from United States, while GB/T 3280 06Cr19Ni10 is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, ASTM A276/A276M S31008 vs GB/T 3280 06Cr19Ni10 is a 81.5% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 54.3%.

Frequently Compared With ASTM A276/A276M S31008:
GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- EN 10088-1 1.4301 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
81.5%
MECHANICAL MATCH
0%
OVERALL
54.3%
Specifications
Property ASTM A276/A276M S31008 GB/T 3280 06Cr19Ni10
Standard ASTM A276/A276M:2017 GB/T 3280-2015
Category Stainless Steel Stainless Steel
C (%) <=0.08 0.08 max
Mn (%) <=2.00 2.00 max
P (%) <=0.045 0.045 max
S (%) <=0.030 0.030 max
Si (%) <=1.50 1.00 max
Cr (%) 24.0-26.0 18.00-20.00
Ni (%) 19.0-22.0 8.00-11.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M S31008 GB/T 3280 06Cr19Ni10
Tensile Strength >=515 MPa 520-720 MPa
Yield Strength >=205 MPa 205-310 MPa
Elongation >=40% 40-60%
Condition Condition A (Annealed), hot-finished, all sizes (first row printed) Not specified
Hardness Not specified 187 HB max
Typical Applications
ASTM A276/A276M S31008
Stainless steel bars and shapes (hot-finished or cold-finished)
GB/T 3280 06Cr19Ni10
Used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.
Can ASTM A276/A276M S31008 Be Substituted With GB/T 3280 06Cr19Ni10?
ASTM A276/A276M S31008 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
ASTM A276/A276M S31008
No active listings currently.
GB/T 3280 06Cr19Ni10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2900–3300 mm (114.17–129.92 in)
On M-EX Right Now
ASTM A276/A276M S31008
0 active listings and RFQs →
GB/T 3280 06Cr19Ni10
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M S31008 and GB/T 3280 06Cr19Ni10?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M S31008 be substituted with GB/T 3280 06Cr19Ni10?
ASTM A276/A276M S31008 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.