ASTM A276/A276M S44400 vs ASTM A240/A240M S44400

Strong Match — 91.7% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M S44400 (ASTM A276/A276M:2017) and ASTM A240/A240M S44400 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M S44400 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while ASTM A240/A240M S44400 is commonly used for pressure vessels and general applications (plate, sheet and strip). ASTM A276/A276M S44400 is defined under ASTM International, originating from United States, while ASTM A240/A240M S44400 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A276/A276M S44400 vs ASTM A240/A240M S44400 is a 100% match. As per mechanical properties, the match is 75%. Combined, this makes them a strong match overall at 91.7%.

Frequently Compared With ASTM A276/A276M S44400:
GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
75%
OVERALL
91.7%
Specifications
Property ASTM A276/A276M S44400 ASTM A240/A240M S44400
Standard ASTM A276/A276M:2017 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.025 <=0.025
Mn (%) <=1.00 <=1.00
P (%) <=0.040 <=0.040
S (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Cr (%) 17.5-19.5 17.5-19.5
Ni (%) <=1.00 <=1.00
Mo (%) 1.75-2.50 1.75-2.50
N (%) <=0.035 <=0.035
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M S44400 ASTM A240/A240M S44400
Tensile Strength >=415 MPa >=415 MPa
Yield Strength >=310 MPa >=275 MPa
Elongation >=20% >=20%
Hardness <=217 HB <=217 HB
Condition Condition A (Annealed), hot-finished, all sizes (first row printed) Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
ASTM A276/A276M S44400
Stainless steel bars and shapes (hot-finished or cold-finished)
ASTM A240/A240M S44400
Pressure vessels and general applications (plate, sheet and strip)
Can ASTM A276/A276M S44400 Be Substituted With ASTM A240/A240M S44400?
ASTM A276/A276M S44400 and ASTM A240/A240M S44400 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S44400 is often considered as a substitute for ASTM A276/A276M S44400 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A276/A276M S44400
0 active listings and RFQs →
ASTM A240/A240M S44400
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M S44400 and ASTM A240/A240M S44400?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M S44400 be substituted with ASTM A240/A240M S44400?
ASTM A276/A276M S44400 and ASTM A240/A240M S44400 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S44400 is often considered as a substitute for ASTM A276/A276M S44400 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.