ASTM A572/A572M Grade 65 vs ASTM A572/A572M Grade 50

Related Material — 66% match based on chemical composition and mechanical property overlap.

ASTM A572/A572M Grade 65 (ASTM A572/A572M:2021) and ASTM A572/A572M Grade 50 (ASTM A572/A572M:2021) are both steel grades. Both fall under the Structural Steel category. ASTM A572/A572M Grade 65 is typically used for riveted or bolted bridge construction, or riveted, bolted or welded construction in other applications, while ASTM A572/A572M Grade 50 is commonly used for riveted, bolted or welded structures. ASTM A572/A572M Grade 65 is defined under ASTM International, originating from United States, while ASTM A572/A572M Grade 50 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A572/A572M Grade 65 vs ASTM A572/A572M Grade 50 is a 99% match. As per mechanical properties, the match is 0%. Combined, this makes them a related material overall at 66%.

Frequently Compared With ASTM A572/A572M Grade 65:
AS/NZS 3679.1 300 CSA G40.21 400W ASTM A1008 SS Grade 50 ASTM A572 Gr.65 GOST 19281 09G2S CSA G40.21 260W CSA G40.21 300W AS/NZS 3679.1 350 CSA G40.21 350W CSA G40.21 400A CSA G40.21 480W ASTM A1008 SS Grade 80
Match Breakdown
CHEMISTRY MATCH
99%
MECHANICAL MATCH
0%
OVERALL
66%
Specifications
Property ASTM A572/A572M Grade 65 ASTM A572/A572M Grade 50
Standard ASTM A572/A572M:2021 ASTM A572/A572M:2021
Category Structural Steel Structural Steel
C (%) <=0.23 <=0.23
Mn (%) <=1.65 <=1.35
P (%) <=0.030 <=0.030
S (%) <=0.030 <=0.030
Si (%) <=0.40 <=0.40
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A572/A572M Grade 65 ASTM A572/A572M Grade 50
Tensile Strength >=550 MPa >=450 MPa
Yield Strength >=450 MPa >=345 MPa
Elongation >=15% >=18%
Condition Tension test per Table 4; one set of minimum values for all product thicknesses; Elongation is in 200 mm gauge length, 50 mm values in the tensile block Tension test per Table 4; one set of minimum values for all product thicknesses; Elongation is in 200 mm gauge length, 50 mm values in the tensile block
Typical Applications
ASTM A572/A572M Grade 65
Riveted or bolted bridge construction, or riveted, bolted or welded construction in other applications
ASTM A572/A572M Grade 50
Riveted, bolted or welded structures
Can ASTM A572/A572M Grade 65 Be Substituted With ASTM A572/A572M Grade 50?
ASTM A572/A572M Grade 65 and ASTM A572/A572M Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
ASTM A572/A572M Grade 65
0 active listings and RFQs →
ASTM A572/A572M Grade 50
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A572/A572M Grade 65 and ASTM A572/A572M Grade 50?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A572/A572M Grade 65 be substituted with ASTM A572/A572M Grade 50?
ASTM A572/A572M Grade 65 and ASTM A572/A572M Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.