Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
ASTM A681 S6 (ASTM A681:2008) and IS 1570 (Part 6) 133T3 (IS 1570 (Part 6):1996) are both steel grades.
Both fall under the Tool & Die Steels category.
ASTM A681 S6 is defined under ASTM International, originating from United States, while IS 1570 (Part 6) 133T3 is defined under Bureau of Indian Standards (IS), originating from India.
As per chemical composition, ASTM A681 S6 vs IS 1570 (Part 6) 133T3 is a 50% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
ASTM A681 S6
IS 1570 (Part 6) 133T3
Hardness
<=229 HB
Not specified
Condition
Annealed (maximum Brinell hardness)
Not specified
Typical Applications
ASTM A681 S6
Tools, dies and fixtures (clause 1.2)
IS 1570 (Part 6) 133T3
Not documented
Key Differences
ASTM A681 S6 specifies V, Mo which are not specified for IS 1570 (Part 6) 133T3.
IS 1570 (Part 6) 133T3 specifies Cu, Ni which are not specified for ASTM A681 S6.
Can ASTM A681 S6 Be Substituted With IS 1570 (Part 6) 133T3?
ASTM A681 S6 and IS 1570 (Part 6) 133T3 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between ASTM A681 S6 and IS 1570 (Part 6) 133T3?
ASTM A681 S6 specifies V, Mo which are not specified for IS 1570 (Part 6) 133T3. IS 1570 (Part 6) 133T3 specifies Cu, Ni which are not specified for ASTM A681 S6.
Can ASTM A681 S6 be substituted with IS 1570 (Part 6) 133T3?
ASTM A681 S6 and IS 1570 (Part 6) 133T3 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.