Strong Match — 88% match based on chemical composition and mechanical property overlap.

ASTM A959 310HCbN (ASTM A959:2011) and EN 10088-1 X6CrNi25-20 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 310HCbN is defined under ASTM International, originating from United States, while EN 10088-1 X6CrNi25-20 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A959 310HCbN vs EN 10088-1 X6CrNi25-20 is a 88% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 88%.

Frequently Compared With ASTM A959 310HCbN:
EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12MoH GB/T 3280 06Cr19Ni10 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H GOST 5632 08X18H10 EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH ASTM A959 .-
Match Breakdown
CHEMISTRY MATCH
88%
MECHANICAL MATCH
No shared data
OVERALL
88%
Specifications
Property ASTM A959 310HCbN EN 10088-1 X6CrNi25-20
Standard ASTM A959:2011 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.04-0.10 0.04-0.08
Cb (%) 0.20-0.60 Not specified
Cr (%) 24.0-26.0 24.0-26.0
Mn (%) <=2.00 <=2.00
N (%) 0.15-0.35 <=0.10
Ni (%) 19.0-22.0 19.0-22.0
P (%) <=0.045 <=0.035
S (%) <=0.030 <=0.015
Si (%) <=1.00 <=0.70
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
ASTM A959 310HCbN
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
EN 10088-1 X6CrNi25-20
Not documented
Key Differences
Can ASTM A959 310HCbN Be Substituted With EN 10088-1 X6CrNi25-20?
ASTM A959 310HCbN and EN 10088-1 X6CrNi25-20 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrNi25-20 is often considered as a substitute for ASTM A959 310HCbN in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A959 310HCbN
0 active listings and RFQs →
EN 10088-1 X6CrNi25-20
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 310HCbN and EN 10088-1 X6CrNi25-20?
ASTM A959 310HCbN specifies Cb which is not specified for EN 10088-1 X6CrNi25-20.
Can ASTM A959 310HCbN be substituted with EN 10088-1 X6CrNi25-20?
ASTM A959 310HCbN and EN 10088-1 X6CrNi25-20 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrNi25-20 is often considered as a substitute for ASTM A959 310HCbN in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.