ASTM A959 317LM vs JIS G4304 SUS317LN

Close Alternative — 82.2% match based on chemical composition and mechanical property overlap.

ASTM A959 317LM (ASTM A959:2011) and JIS G4304 SUS317LN (JIS G4304:2021) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 317LM is typically used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1), while JIS G4304 SUS317LN is commonly used for hot-rolled stainless steel plates and strips. ASTM A959 317LM is defined under ASTM International, originating from United States, while JIS G4304 SUS317LN is defined under Japanese Industrial Standards (JIS), originating from Japan.

As per chemical composition, ASTM A959 317LM vs JIS G4304 SUS317LN is a 82.2% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 82.2%.

Frequently Compared With ASTM A959 317LM:
ASTM A959 2304 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoH GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4301 EN 10088-1 1.4401
Match Breakdown
CHEMISTRY MATCH
82.2%
MECHANICAL MATCH
No shared data
OVERALL
82.2%
Specifications
Property ASTM A959 317LM JIS G4304 SUS317LN
Standard ASTM A959:2011 JIS G4304:2021
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Cr (%) 18.0-20.0 18.00-20.00
Mn (%) <=2.00 <=2.00
Mo (%) 4.0-5.0 3.00-4.00
N (%) <=0.20 0.10-0.22
Ni (%) 13.5-17.5 11.00-15.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A959 317LM JIS G4304 SUS317LN
Tensile Strength Not specified >=550 MPa
Yield Strength Not specified >=245 MPa
Elongation Not specified >=40%
Hardness Not specified <=217 HB
Condition Not specified Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser
Typical Applications
ASTM A959 317LM
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
JIS G4304 SUS317LN
Hot-rolled stainless steel plates and strips
Can ASTM A959 317LM Be Substituted With JIS G4304 SUS317LN?
ASTM A959 317LM and JIS G4304 SUS317LN are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
ASTM A959 317LM
0 active listings and RFQs →
JIS G4304 SUS317LN
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 317LM and JIS G4304 SUS317LN?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A959 317LM be substituted with JIS G4304 SUS317LN?
ASTM A959 317LM and JIS G4304 SUS317LN are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.