ASTM A959 436 vs EN 10088-1 X6CrMoNb17-1

Strong Match — 92.2% match based on chemical composition and mechanical property overlap.

ASTM A959 436 (ASTM A959:2011) and EN 10088-1 X6CrMoNb17-1 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 436 is defined under ASTM International, originating from United States, while EN 10088-1 X6CrMoNb17-1 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A959 436 vs EN 10088-1 X6CrMoNb17-1 is a 92.2% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 92.2%.

Frequently Compared With ASTM A959 436:
GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 11Cr17Ni13W3TiH GOST 5632 08X18H10 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- GOST 5632 06Kh23N28 EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
92.2%
MECHANICAL MATCH
No shared data
OVERALL
92.2%
Specifications
Property ASTM A959 436 EN 10088-1 X6CrMoNb17-1
Standard ASTM A959:2011 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.12 <=0.08
Cr (%) 16.0-18.0 16.0-18.0
Mn (%) <=1.00 <=1.00
Mo (%) 0.75-1.25 0.80-1.40
P (%) <=0.040 <=0.040
S (%) <=0.030 <=0.015
Si (%) <=1.00 <=1.00
N (%) Not specified <=0.040
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
ASTM A959 436
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
EN 10088-1 X6CrMoNb17-1
Not documented
Key Differences
Can ASTM A959 436 Be Substituted With EN 10088-1 X6CrMoNb17-1?
ASTM A959 436 and EN 10088-1 X6CrMoNb17-1 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrMoNb17-1 is often considered as a substitute for ASTM A959 436 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A959 436
0 active listings and RFQs →
EN 10088-1 X6CrMoNb17-1
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 436 and EN 10088-1 X6CrMoNb17-1?
EN 10088-1 X6CrMoNb17-1 specifies N which is not specified for ASTM A959 436.
Can ASTM A959 436 be substituted with EN 10088-1 X6CrMoNb17-1?
ASTM A959 436 and EN 10088-1 X6CrMoNb17-1 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrMoNb17-1 is often considered as a substitute for ASTM A959 436 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.