ASTM A959:2011 800: Austenitic stainless steel type 800 (UNS N08800) with the composition limits of ASTM A959-11. Carbon up to 0.10% and chromium 19.0-23.0%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
Al
C
Cr
Cu
Fe
Mn
Ni
P
S
Si
Ti
0.15-0.60
<=0.10
19.0-23.0
<=0.75
>=39.5
<=1.50
30.0-35.0
<=0.045
<=0.015
<=1.00
0.15-0.60
More data from ASTM A959:2011
From the standard
Other composition limitsfrom Table 1 and its footnotes
UNS number
N08800
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
800 (common type number, not a trademark, widely used; not associated with any one product)
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Fe 39.5 min, Al 0.15-0.60, Ti 0.15-0.60
Iron
Determined arithmetically by difference of 100 minus the sum of the other specified elements (footnote F)
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes
Active ASTM A959:2011 800 Listings on M-EX (For Sale)