ASTM A959 904L vs ASTM A240/A240M N08904

Strong Match — 99.3% match based on chemical composition and mechanical property overlap.

ASTM A959 904L (ASTM A959:2011) and ASTM A240/A240M N08904 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 904L is typically used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1), while ASTM A240/A240M N08904 is commonly used for pressure vessels and general applications (plate, sheet and strip). ASTM A959 904L is defined under ASTM International, originating from United States, while ASTM A240/A240M N08904 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A959 904L vs ASTM A240/A240M N08904 is a 99.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 99.3%.

Frequently Compared With ASTM A959 904L:
EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr13H GB/T 3280 06Cr19Ni10 ASTM A959 .- GOST 5632 06Kh23N28 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
99.3%
MECHANICAL MATCH
No shared data
OVERALL
99.3%
Specifications
Property ASTM A959 904L ASTM A240/A240M N08904
Standard ASTM A959:2011 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Cr (%) 19.0-23.0 19.0-23.0
Cu (%) 1.00-2.00 1.00-2.00
Mn (%) <=2.00 <=2.00
Mo (%) 4.0-5.0 4.00-5.00
N (%) <=0.10 <=0.10
Ni (%) 23.0-28.0 23.0-28.0
P (%) <=0.040 <=0.045
S (%) <=0.030 <=0.035
Si (%) <=1.00 <=1.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A959 904L ASTM A240/A240M N08904
Tensile Strength Not specified >=490 MPa
Yield Strength Not specified >=220 MPa
Elongation Not specified >=35%
Hardness Not specified <=90 HRBW
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
ASTM A959 904L
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
ASTM A240/A240M N08904
Pressure vessels and general applications (plate, sheet and strip)
Can ASTM A959 904L Be Substituted With ASTM A240/A240M N08904?
ASTM A959 904L and ASTM A240/A240M N08904 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08904 is often considered as a substitute for ASTM A959 904L in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A959 904L
0 active listings and RFQs →
ASTM A240/A240M N08904
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 904L and ASTM A240/A240M N08904?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A959 904L be substituted with ASTM A240/A240M N08904?
ASTM A959 904L and ASTM A240/A240M N08904 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08904 is often considered as a substitute for ASTM A959 904L in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.