ASTM A959:2011 S35125: Austenitic stainless steel grade (UNS S35125) with the composition limits of ASTM A959-11. Carbon up to 0.10% and chromium 20.0-23.0%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Cb
Cr
Mn
Mo
Ni
P
S
Si
<=0.10
0.25-0.60
20.0-23.0
1.00-1.50
2.00-3.00
31.0-35.0
<=0.045
<=0.015
<=0.50
More data from ASTM A959:2011
From the standard
Other composition limitsfrom Table 1 and its footnotes
UNS number
S35125
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Cb 0.25-0.60
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes
Active ASTM A959:2011 S35125 Listings on M-EX (For Sale)