ASTM A959 S35315 vs EN 10088-1 X6NiCrSiNCe35-25

Strong Match — 96.9% match based on chemical composition and mechanical property overlap.

ASTM A959 S35315 (ASTM A959:2011) and EN 10088-1 X6NiCrSiNCe35-25 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 S35315 is defined under ASTM International, originating from United States, while EN 10088-1 X6NiCrSiNCe35-25 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A959 S35315 vs EN 10088-1 X6NiCrSiNCe35-25 is a 96.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 96.9%.

Frequently Compared With ASTM A959 S35315:
GB/T 3280 06Cr19Ni10 EN 10088-1 1.4845 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoH ASTM A959 .-
Match Breakdown
CHEMISTRY MATCH
96.9%
MECHANICAL MATCH
No shared data
OVERALL
96.9%
Specifications
Property ASTM A959 S35315 EN 10088-1 X6NiCrSiNCe35-25
Standard ASTM A959:2011 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) 0.04-0.08 0.04-0.08
Ce (%) 0.03-0.10 0.03-0.08
Cr (%) 24.0-26.0 24.0-26.0
Mn (%) <=2.00 <=2.00
N (%) 0.12-0.18 0.12-0.20
Ni (%) 34.0-36.0 34.0-36.0
P (%) <=0.045 <=0.040
S (%) <=0.030 <=0.015
Si (%) 1.20-2.00 1.20-2.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
ASTM A959 S35315
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
EN 10088-1 X6NiCrSiNCe35-25
Not documented
Can ASTM A959 S35315 Be Substituted With EN 10088-1 X6NiCrSiNCe35-25?
ASTM A959 S35315 and EN 10088-1 X6NiCrSiNCe35-25 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6NiCrSiNCe35-25 is often considered as a substitute for ASTM A959 S35315 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A959 S35315
0 active listings and RFQs →
EN 10088-1 X6NiCrSiNCe35-25
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 S35315 and EN 10088-1 X6NiCrSiNCe35-25?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A959 S35315 be substituted with EN 10088-1 X6NiCrSiNCe35-25?
ASTM A959 S35315 and EN 10088-1 X6NiCrSiNCe35-25 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6NiCrSiNCe35-25 is often considered as a substitute for ASTM A959 S35315 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.