BS 970 (Part 1):1983 430S17 Steel: Specifications & Listings

BS 970 (Part 1):1983 430S17: 430S17 is a ferritic stainless steel grade specified in BS 970 Part 1:1983 (Table 13, category 1).

Category: Stainless Steel
Grade Details
GradeBS 970 (Part 1):1983 430S17
Standard BS 970 (Part 1):1983
ApplicationsStainless and heat resisting steel for mechanical and allied engineering purposes (Table 13).
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
BS 970 EN60 BS 970:1955 UK No activity yet
ASTM A959 430Ti ASTM A959:2011 USA No activity yet
BS 970 (Part 1) 430S17 BS 970 (Part 1):1991 UK No activity yet
ASTM A240/A240M S43000 ASTM A240/A240M:2025 USA No activity yet
IS 5522 X07Cr17 IS 5522:2014 India No activity yet
JIS G4304 SUS430 JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 (Part 1) 430S17 BS 970 (Part 1):1991 Strong Match
BS 970 (Part 3) 430S17 BS 970 (Part 3):1991 Strong Match
IS 1570 (Part 5) X07Cr17 IS 1570 (Part 5):1985 Strong Match
IS 6911 X07Cr17 IS 6911:1992 Strong Match
BS 970 EN60 BS 970:1955 Strong Match
ASTM A240/A240M S43000 ASTM A240/A240M:2025 Strong Match
IS 5522 X07Cr17 IS 5522:2014 Strong Match
JIS G4304 SUS430 JIS G4304:2021 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Cr Ni
<=0.08 <=1.0 <=1.0 <=0.040 <=0.030 16.0-18.0 <=0.50

More data from BS 970 (Part 1):1983

From the standard
Mechanical properties by heat treatment condition
ConditionLimiting ruling section (mm)Heat treatmentRm (N/mm2)Re min (N/mm2)A min (%)Izod min (ft lbf)KCV min (J)Rp0.2 min (N/mm2), when specifically orderedHB
Not lettered63Anneal 750-820 deg C, cooled freely in air (note 32)430 min28020--245170 max
All Table 13 steels are category 1. Rp0.2 applies when specifically ordered (note 10). 1 N/mm2 = 1 MPa.
Source: BS 970 (Part 1):1983, Table 13
Hardness, softened condition
Hardness HB, softened condition
170 max
Source: BS 970 (Part 1):1983, Table 13
Comparison with earlier editions
BS 970:1970/72 designation
430S15
BS 970:1955 En No.
60
Appendix D note 47: where a comparison is made the steels are not necessarily equivalent. 'Not listed' means the earlier edition has no entry under this designation.
Source: BS 970 (Part 1):1983, Appendix D

Active BS 970 (Part 1):1983 430S17 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970 (Part 1):1983 430S17 listings at this time.

Register for Alerts

Buyer RFQs for BS 970 (Part 1):1983 430S17

+ Post an RFQ for this grade

No open buyer requirements for BS 970 (Part 1):1983 430S17 at this time.

Register for Alerts