BS 970 (Part 1):1983 835H15 Steel: Specifications & Listings

BS 970 (Part 1):1983 835H15: 835H15 is a case hardening alloy steel grade supplied to hardenability (H) requirements, specified in BS 970 Part 1:1983 (Table 10, category 1).

Category: Alloy Steel
Grade Details
GradeBS 970 (Part 1):1983 835H15
Standard BS 970 (Part 1):1983
ApplicationsCase hardening steel supplied to specified hardenability limits (end quench test, Table 10).
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
BS 970 (Part 1) 835H15 BS 970 (Part 1):1991 UK No activity yet
BS 970 (Part 1) 835M15 BS 970 (Part 1):1991 UK No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 (Part 1) 835M15 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 1) 835H15 BS 970 (Part 1):1991 Strong Match
BS 970 (Part 1) 835M15 BS 970 (Part 1):1991 Strong Match
BS 970 (Part 3) 835M15 BS 970 (Part 3):1991 Strong Match
BS 970 EN39B BS 970:1955 Close Alternative
BS 970 (Part 1) 835M30 BS 970 (Part 1):1983 Close Alternative
BS 970 EN30B BS 970:1955 Close Alternative
BS 970 (Part 1) 832M13 BS 970 (Part 1):1983 Close Alternative
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Mn Cr Mo Ni P S
0.12-0.18 0.25-0.50 1.00-1.40 0.15-0.30 3.90-4.30 <=0.035 <=0.040

More data from BS 970 (Part 1):1983

From the standard
Other composition limits
Phosphorus and sulphur
P 0.035 max, S 0.040 max, alloy steels (clause 1.7.2.1)
Residual elements: see clause 1.7.3.
Source: BS 970 (Part 1):1983, clause 1.7.2.1
Heat treatment and maximum hardness
Preheat treatment temperature (hardenability test)
880-900 deg C
Austenitizing temperature (hardenability test)
830 deg C
Maximum hardness HB, bars and billets for forging
277
Maximum hardness HB, forgings and bars for machining, sub-critically annealed
277
Maximum hardness HB, forgings and bars for machining, normalized and tempered
269
Maximum hardness values apply when specified on the order, in the condition of delivery. Quantities not limited in Table 12 are not shown.
Source: BS 970 (Part 1):1983, Table 12
Hardenability requirements (end quench test)
Distance from quenched end (mm)HRC maxHRC min
1.54538
34538
54538
74538
94538
114538
134538
154538
204537
254536
304435
354434
404433
454332
Rockwell C hardness at the stated distance from the quenched end in the end quench hardenability test. A dash means no value is specified. Preheat and austenitizing temperatures: see the heat treatment block.
Source: BS 970 (Part 1):1983, Table 10
Comparison with earlier editions
BS 970:1970/72 designation
835H15
BS 970:1955 En No.
None
Appendix D note 47: where a comparison is made the steels are not necessarily equivalent. 'Not listed' means the earlier edition has no entry under this designation.
Source: BS 970 (Part 1):1983, Appendix D

Active BS 970 (Part 1):1983 835H15 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970 (Part 1):1983 835H15 listings at this time.

Register for Alerts

Buyer RFQs for BS 970 (Part 1):1983 835H15

+ Post an RFQ for this grade

No open buyer requirements for BS 970 (Part 1):1983 835H15 at this time.

Register for Alerts