BS 970 EN100E vs BS 970 EN100

Strong Match — 94.3% match based on chemical composition and mechanical property overlap.

BS 970 EN100E (BS 970:1955) and BS 970 EN100 (BS 970:1955) are both steel grades. Both fall under the Alloy Steel category. BS 970 EN100E is defined under British Standards (BS), originating from United Kingdom, while BS 970 EN100 is defined under British Standards (BS), originating from United Kingdom.

As per chemical composition, BS 970 EN100E vs BS 970 EN100 is a 91.4% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 94.3%.

Frequently Compared With BS 970 EN100E:
IS 4367 07Cr4Mo6 IS 1570 (Part 4) 07Cr4Mo6 NF A35-565 100C6 UNI 11234 100Cr6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 4) 105Cr5 IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 7) 10Cr36Mo10H IS 4367 10Cr9Mo10 IS 1570 (Part 4) 10Mo6 IS 1570 (Part 7) 10Mo6H
Match Breakdown
CHEMISTRY MATCH
91.4%
MECHANICAL MATCH
100%
OVERALL
94.3%
Specifications
Property BS 970 EN100E BS 970 EN100
Standard BS 970:1955 BS 970:1955
Category Alloy Steel Alloy Steel
C (%) 0.25-0.35 0.35-0.45
Si (%) <=0.50 <=0.50
Mn (%) 1.20-1.50 1.20-1.50
Ni (%) 0.50-1.00 0.50-1.00
Cr (%) 0.30-0.60 0.30-0.60
Mo (%) 0.15-0.25 0.15-0.25
S (%) <=0.050 <=0.050
P (%) <=0.050 <=0.050
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property BS 970 EN100E BS 970 EN100
Tensile Strength ≥695 MPa (45 tons/sq in, converted) ≥695 MPa (45 tons/sq in, converted)
Yield Strength ≥525 MPa (34 tons/sq in, converted) ≥525 MPa (34 tons/sq in, converted)
Elongation ≥22% ≥22%
Hardness 201-255 HB 201-255 HB
Condition Hardened and tempered R, ruling section 6 in (lowest-strength condition of the standard) Hardened and tempered R, ruling section 6 in (lowest-strength condition of the standard)
Typical Applications
BS 970 EN100E
Not documented
BS 970 EN100
Bars and billets for forging; forgings and drop-forgings; bars for machining; bright bars. Suitable for 45/55 (R), 50/60 (S), 55/65 (T), 60/70 (U), 65/75 (V) tons/sq in according to ruling section. Capable of meeting the test requirements of En 16 and En 19 except where used for special purposes.
Can BS 970 EN100E Be Substituted With BS 970 EN100?
BS 970 EN100E and BS 970 EN100 overlap closely enough on chemistry and mechanical properties that BS 970 EN100 is often considered as a substitute for BS 970 EN100E in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
BS 970 EN100E
0 active listings and RFQs →
BS 970 EN100
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between BS 970 EN100E and BS 970 EN100?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can BS 970 EN100E be substituted with BS 970 EN100?
BS 970 EN100E and BS 970 EN100 overlap closely enough on chemistry and mechanical properties that BS 970 EN100 is often considered as a substitute for BS 970 EN100E in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.