Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Si
Mn
Mo
S
P
0.30-0.40
<=0.25
1.30-1.80
0.20-0.35
0.12-0.20
<=0.060
More data from BS 970:1955
From the standard
Condition of material on delivery
A
Bars and billets for forging as rolled or forged unless order states otherwise.
B
Forgings and drop-forgings finally heat treated unless order states otherwise.
C
Bars for machining finally heat treated unless order states otherwise.
D
Bright bars finally heat treated, before or after cold work at manufacturer option, unless order states otherwise.
Source: BS 970:1955, Part 2, En 16M (page 87)
Other tests and requirements
If required, mechanical properties shall be agreed between purchaser and manufacturer.
Source: BS 970:1955, Part 2, En 16M
Heat treatment
Harden (oil)
830/860 C
Temper
suitable temperature between 550 C and 660 C
Temperatures in degrees C as printed.
Source: BS 970:1955, Part 2, En 16M (page 87)
Status in the 1955 edition
Status
Deleted by Amendment 7
Reason
Amendment 7 (Sep 1970): direct hardening alloy steels moved to BS 970 Part 2:1970
BS 970:1955 was amended up to Amendment 10 (June 1972); steels were moved to the revised Parts 1 to 5 and deleted from this edition.
Source: BS 970:1955, Amendment slips 6 to 10