BS 970:1955 EN355 Steel: Specifications & Listings

BS 970:1955 EN355: EN355: 2 per cent nickel-chromium-molybdenum case-hardening steel (low chromium). Specified in BS 970:1955, Part 2.

Category: Alloy Steel
Grade Details
GradeBS 970:1955 EN355
Standard BS 970:1955
ApplicationsBars and billets for forging; forgings and drop-forgings; bars for machining; bright bars. Suitable for tensile strength 85 tons/sq in min.
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
BS 970 (Part 1) 822M17 BS 970 (Part 1):1983 UK No activity yet
BS 970 (Part 1) 822H17 BS 970 (Part 1):1991 UK No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
IS 11169 (Part 1) 16Ni8Cr6Mo2 IS 11169 (Part 1):2022 Strong Match
BS 970 (Part 3) 822M17 BS 970 (Part 3):1991 Strong Match
BS 970 (Part 1) 822H17 BS 970 (Part 1):1991 Strong Match
BS 970 (Part 1) 822M17 BS 970 (Part 1):1983 Close Alternative
BS 970 (Part 1) 822H17 BS 970 (Part 1):1983 Close Alternative
IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 4):1988 Related Material
BS 970 EN39B BS 970:1955 Related Material
BS 970 (Part 3) 805M17 BS 970 (Part 3):1991 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn Ni Cr Mo S P
<=0.20 <=0.35 0.40-0.70 1.80-2.20 1.40-1.70 0.15-0.25 <=0.050 <=0.050
Mechanical Properties
Tensile Strength ≥1313 MPa (85 tons/sq in, converted)
Elongation ≥12%
Condition core, min (lowest-strength condition of the standard)

More data from BS 970:1955

From the standard
Condition of material on delivery
A
Bars and billets for forging as rolled or forged.
B
Forgings and drop-forgings in the softened condition.
C
Bars for machining in the softened condition.
D
Bright bars cold worked, condition suitable for machining; max Brinell may be agreed.
Source: BS 970:1955, Part 2, En 355 (page 200)
Mechanical properties
ConditionRuling section or size (in)Tensile strength (tons/sq in)Yield stress (tons/sq in)Elongation (%)Izod impact (ft lb)Brinell (HB)Proof stress 0.2% (tons/sq in), when requested
core, min-85-1225--
softened, max-----<=277-
Values as printed in BS 970:1955; tensile strength, yield stress and proof stress in tons/sq in, Izod in ft lb. Minimum unless a range is shown.
Source: BS 970:1955, Part 2, En 355 (page 201)
Heat treatment
Blank carburise (1 1/8 in diameter test bars)
880/930 C
Refine (1 1/8 in diameter test bars)
850/880 C, cool in air or oil
Harden (oil) (1 1/8 in diameter test bars)
780/820 C
Temper
not exceeding 200 C
Temperatures in degrees C as printed.
Source: BS 970:1955, Part 2, En 355 (page 200)
Notes
Note
See Appendix A for single quench; by arrangement tests on samples without blank carburising or with short heating.
Source: BS 970:1955, Part 2, En 355
Status in the 1955 edition
Status
Deleted by Amendment 8
Reason
Amendment 8 (Jul 1971): alloy case hardening steels moved to BS 970 Part 3:1971
BS 970:1955 was amended up to Amendment 10 (June 1972); steels were moved to the revised Parts 1 to 5 and deleted from this edition.
Source: BS 970:1955, Amendment slips 6 to 10

Active BS 970:1955 EN355 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970:1955 EN355 listings at this time.

Register for Alerts

Buyer RFQs for BS 970:1955 EN355

+ Post an RFQ for this grade

No open buyer requirements for BS 970:1955 EN355 at this time.