Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
BS 970 EN49A (BS 970:1955) and IS 5517 55Cr3 (IS 5517:1993) are both steel grades.
Both fall under the Spring Steel category.
BS 970 EN49A is defined under British Standards (BS), originating from United Kingdom, while IS 5517 55Cr3 is defined under Bureau of Indian Standards (IS), originating from India.
As per chemical composition, BS 970 EN49A vs IS 5517 55Cr3 is a 75.5% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
BS 970 EN49A
IS 5517 55Cr3
Tensile Strength
Not specified
900-1050 MPa
Yield Strength (0.2% proof)
Not specified
660 MPa min
Elongation
Not specified
>=12%
Izod Impact
Not specified
35 J min
Hardness (annealed)
Not specified
<=220 HB
Condition
Not specified
Hardened and tempered, ruling section up to 63 mm
Key Differences
IS 5517 55Cr3 specifies Cr which is not specified for BS 970 EN49A.
Can BS 970 EN49A Be Substituted With IS 5517 55Cr3?
BS 970 EN49A and IS 5517 55Cr3 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between BS 970 EN49A and IS 5517 55Cr3?
IS 5517 55Cr3 specifies Cr which is not specified for BS 970 EN49A.
Can BS 970 EN49A be substituted with IS 5517 55Cr3?
BS 970 EN49A and IS 5517 55Cr3 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.