BS 970:1955 EN55 Steel: Specifications & Listings

BS 970:1955 EN55: EN55: High chromium-nickel-tungsten valve steel. Specified in BS 970:1955, Part 2.

Category: Stainless Steel
Grade Details
GradeBS 970:1955 EN55
Standard BS 970:1955
ApplicationsBars and billets for forging; forgings and drop-forgings; bars for machining; bright bars.
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 EN54 BS 970:1955 Close Alternative
IS 1570 (Part 5) X40Ni14Cr14W3Si2 IS 1570 (Part 5):1985 Related Material
BS 970 EN56D BS 970:1955 Related Material
JIS G4304 SUS420J2 JIS G4304:2021 Related Material
JIS G4305 SUS420J2 JIS G4305:2012 Related Material
IS 1570 (Part 5) X20Cr21Ni12N IS 1570 (Part 5):1985 Related Material
IS 1570 (Part 7) 7Cr18Ni10H IS 1570 (Part 7):1992 Related Material
BS 970 EN56C BS 970:1955 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn Ni Cr W S P
0.18-0.45 1.00-2.50 <=1.00 6.00-12.0 >=17.0 2.00-4.00 <=0.045 <=0.045

More data from BS 970:1955

From the standard
Condition of material on delivery
A
Bars and billets for forging as rolled or forged unless order states otherwise.
B
Forgings and drop-forgings finally heat treated unless order states otherwise.
C
Bars for machining finally heat treated unless order states otherwise.
D
Bright bars in the condition stated on the order.
Source: BS 970:1955, Part 2, En 55 (page 163)
Mechanical properties
ConditionRuling section or size (in)Tensile strength (tons/sq in)Yield stress (tons/sq in)Elongation (%)Izod impact (ft lb)Brinell (HB)Proof stress 0.2% (tons/sq in), when requested
----20<=302-
Values as printed in BS 970:1955; tensile strength, yield stress and proof stress in tons/sq in, Izod in ft lb. Minimum unless a range is shown.
Source: BS 970:1955, Part 2, En 55 (page 163)
Other tests and requirements
Mechanical Test Samples
Test samples from bars and billets for forging over 1 1/8 in diameter forged or machined to 1 1/8 in diameter and heat treated in that size; bars of 1 1/8 in diameter and under heat treated in full size. Test pieces from forgings and bars for machining selected as in the general clauses.
Source: BS 970:1955, Part 2, En 55
Heat treatment
Soften
cooling freely in air or quenching in oil or water (at manufacturer option) from 950/1020 C
Temperatures in degrees C as printed.
Source: BS 970:1955, Part 2, En 55 (page 163)
Status in the 1955 edition
Status
Deleted by Amendment 6
Reason
Amendment 6 (Feb 1970): stainless, heat resisting and valve steels moved to BS 970 Part 4:1970
BS 970:1955 was amended up to Amendment 10 (June 1972); steels were moved to the revised Parts 1 to 5 and deleted from this edition.
Source: BS 970:1955, Amendment slips 6 to 10

Active BS 970:1955 EN55 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970:1955 EN55 listings at this time.

Register for Alerts

Buyer RFQs for BS 970:1955 EN55

+ Post an RFQ for this grade

No open buyer requirements for BS 970:1955 EN55 at this time.

Register for Alerts