BS 970 EN56C vs BS 970 EN56D

Strong Match — 94.4% match based on chemical composition and mechanical property overlap.

BS 970 EN56C (BS 970:1955) and BS 970 EN56D (BS 970:1955) are both steel grades. Both fall under the Stainless Steel category. BS 970 EN56C is defined under British Standards (BS), originating from United Kingdom, while BS 970 EN56D is defined under British Standards (BS), originating from United Kingdom.

As per chemical composition, BS 970 EN56C vs BS 970 EN56D is a 91.7% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 94.4%.

Frequently Compared With BS 970 EN56C:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
91.7%
MECHANICAL MATCH
100%
OVERALL
94.4%
Specifications
Property BS 970 EN56C BS 970 EN56D
Standard BS 970:1955 BS 970:1955
Category Stainless Steel Stainless Steel
C (%) 0.18-0.25 0.25-0.35
Si (%) <=1.00 <=1.00
Mn (%) <=1.00 <=1.00
Ni (%) <=1.00 <=1.00
Cr (%) 12.0-14.0 12.0-14.0
S (%) <=0.045 <=0.045
P (%) <=0.045 <=0.045
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property BS 970 EN56C BS 970 EN56D
Tensile Strength ≥541 MPa (35 tons/sq in, converted) ≥541 MPa (35 tons/sq in, converted)
Yield Strength ≥386 MPa (25 tons/sq in, converted) ≥386 MPa (25 tons/sq in, converted)
Elongation ≥25% ≥25%
Hardness 152-207 HB 152-207 HB
Condition Hardened and tempered P (ruling 6), ruling section 6 in (lowest-strength condition of the standard) Hardened and tempered P (ruling 6), ruling section 6 in (lowest-strength condition of the standard)
Can BS 970 EN56C Be Substituted With BS 970 EN56D?
BS 970 EN56C and BS 970 EN56D overlap closely enough on chemistry and mechanical properties that BS 970 EN56D is often considered as a substitute for BS 970 EN56C in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
BS 970 EN56C
0 active listings and RFQs →
BS 970 EN56D
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between BS 970 EN56C and BS 970 EN56D?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can BS 970 EN56C be substituted with BS 970 EN56D?
BS 970 EN56C and BS 970 EN56D overlap closely enough on chemistry and mechanical properties that BS 970 EN56D is often considered as a substitute for BS 970 EN56C in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.