Strong Match — 90.9% match
based on chemical composition and mechanical property overlap.
BS 970 EN58E (BS 970:1955) and ASTM A959 SS304 (ASTM A959:2011) are both steel grades.
Both fall under the Stainless Steel category.
BS 970 EN58E is defined under British Standards (BS), originating from United Kingdom, while ASTM A959 SS304 is defined under ASTM International, originating from United States.
As per chemical composition, BS 970 EN58E vs ASTM A959 SS304 is a 90.9% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a strong match overall at 90.9%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
BS 970 EN58E
ASTM A959 SS304
Tensile Strength
≥541 MPa (35 tons/sq in, converted)
Not specified
Yield Strength
≥185 MPa (12 tons/sq in, converted)
Not specified
Elongation
≥30%
Not specified
Condition
, ruling section 6 in (lowest-strength condition of the standard)
Not specified
Typical Applications
BS 970 EN58E
Not documented
ASTM A959 SS304
Food processing, chemical equipment, kitchen equipment
Can BS 970 EN58E Be Substituted With ASTM A959 SS304?
BS 970 EN58E and ASTM A959 SS304 overlap closely enough on chemistry and mechanical properties that ASTM A959 SS304 is often considered as a substitute for BS 970 EN58E in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
What is the difference between BS 970 EN58E and ASTM A959 SS304?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can BS 970 EN58E be substituted with ASTM A959 SS304?
BS 970 EN58E and ASTM A959 SS304 overlap closely enough on chemistry and mechanical properties that ASTM A959 SS304 is often considered as a substitute for BS 970 EN58E in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.