Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
BS 970 EN58J (BS 970:1955) and GB/T 3280 06Cr19Ni10 (GB/T 3280-2015) are both steel grades.
Both fall under the Stainless Steel category.
BS 970 EN58J is defined under British Standards (BS), originating from United Kingdom, while GB/T 3280 06Cr19Ni10 is defined under Guobiao Standards (GB/T), originating from China.
As per chemical composition, BS 970 EN58J vs GB/T 3280 06Cr19Ni10 is a 77.6% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
BS 970 EN58J
GB/T 3280 06Cr19Ni10
Tensile Strength
≥541 MPa (35 tons/sq in, converted)
520-720 MPa
Yield Strength
≥185 MPa (12 tons/sq in, converted)
205-310 MPa
Elongation
≥30%
40-60%
Condition
, ruling section 6 in (lowest-strength condition of the standard)
Not specified
Hardness
Not specified
187 HB max
Typical Applications
BS 970 EN58J
Not documented
GB/T 3280 06Cr19Ni10
Used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.
Key Differences
BS 970 EN58J specifies Mo which is not specified for GB/T 3280 06Cr19Ni10.
Can BS 970 EN58J Be Substituted With GB/T 3280 06Cr19Ni10?
BS 970 EN58J and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between BS 970 EN58J and GB/T 3280 06Cr19Ni10?
BS 970 EN58J specifies Mo which is not specified for GB/T 3280 06Cr19Ni10.
Can BS 970 EN58J be substituted with GB/T 3280 06Cr19Ni10?
BS 970 EN58J and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.