BS 970 (Part 3) 304S31 vs NF A35-574 Z7CN18-09

Strong Match — 97.6% match based on chemical composition and mechanical property overlap.

BS 970 (Part 3) 304S31 (BS 970 (Part 3):1991) and NF A35-574 Z7CN18-09 (NF A35-574:1990) are both steel grades. Both fall under the Stainless Steel category. BS 970 (Part 3) 304S31 is typically used for bright cold finished bars (cold drawn, turned or precision ground) for general engineering purposes, in straight lengths; austenitic stainless and heat resisting steel (table 18), while NF A35-574 Z7CN18-09 is commonly used for used for food processing equipment, kitchen equipment, chemical tanks, piping, architectural components, and fasteners.. BS 970 (Part 3) 304S31 is defined under British Standards (BS), originating from United Kingdom, while NF A35-574 Z7CN18-09 is defined under Association Francaise de Normalisation (NF), originating from France.

As per chemical composition, BS 970 (Part 3) 304S31 vs NF A35-574 Z7CN18-09 is a 97.6% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 97.6%.

Frequently Compared With BS 970 (Part 3) 304S31:
GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr13H ASTM A959 .- GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
97.6%
MECHANICAL MATCH
No shared data
OVERALL
97.6%
Specifications
Property BS 970 (Part 3) 304S31 NF A35-574 Z7CN18-09
Standard BS 970 (Part 3):1991 NF A35-574:1990
Category Stainless Steel Stainless Steel
C (%) <=0.07 0.08 max
Si (%) <=1.0 1.00 max
Mn (%) <=2.0 2.00 max
P (%) <=0.045 0.045 max
S (%) <=0.030 0.030 max
Cr (%) 17.0-19.0 17.00-19.00
Ni (%) 8.0-11.0 8.00-10.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property BS 970 (Part 3) 304S31 NF A35-574 Z7CN18-09
Tensile Strength Not specified 500-700 MPa
Yield Strength Not specified 190-250 MPa
Elongation Not specified 40-55%
Hardness Not specified 140-210 HB
Typical Applications
BS 970 (Part 3) 304S31
Bright cold finished bars (cold drawn, turned or precision ground) for general engineering purposes, in straight lengths; austenitic stainless and heat resisting steel (Table 18)
NF A35-574 Z7CN18-09
Used for food processing equipment, kitchen equipment, chemical tanks, piping, architectural components, and fasteners.
Can BS 970 (Part 3) 304S31 Be Substituted With NF A35-574 Z7CN18-09?
BS 970 (Part 3) 304S31 and NF A35-574 Z7CN18-09 overlap closely enough on chemistry and mechanical properties that NF A35-574 Z7CN18-09 is often considered as a substitute for BS 970 (Part 3) 304S31 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
Forms & Sizes Available on M-EX
BS 970 (Part 3) 304S31
No active listings currently.
NF A35-574 Z7CN18-09
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2600–2900 mm (102.36–114.17 in)
On M-EX Right Now
BS 970 (Part 3) 304S31
0 active listings and RFQs →
NF A35-574 Z7CN18-09
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between BS 970 (Part 3) 304S31 and NF A35-574 Z7CN18-09?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can BS 970 (Part 3) 304S31 be substituted with NF A35-574 Z7CN18-09?
BS 970 (Part 3) 304S31 and NF A35-574 Z7CN18-09 overlap closely enough on chemistry and mechanical properties that NF A35-574 Z7CN18-09 is often considered as a substitute for BS 970 (Part 3) 304S31 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.