Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
EN 10025-3 S460N (EN 10025-3:2019) and ASTM A572 Gr.65 (ASTM A572) are both steel grades.
Both fall under the Structural Steel category.
EN 10025-3 S460N is defined under European Standard (EN), originating from Europe, while ASTM A572 Gr.65 is defined under ASTM International, originating from United States.
As per chemical composition, EN 10025-3 S460N vs ASTM A572 Gr.65 is a 62.5% match.
As per mechanical properties, the match is 25.9%.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10025-3 S460N
ASTM A572 Gr.65
Tensile Strength
540-720 MPa
550-690 MPa
Yield Strength
>=460 MPa
450 MPa min
Elongation
>=17%
18-21%
Condition
Normalized or normalized rolled (N), nominal thickness up to 16 mm (tensile strength up to 100 mm), Table 4
Not specified
Hardness
Not specified
170-220 HB
Typical Applications
EN 10025-3 S460N
Not documented
ASTM A572 Gr.65
Used for bridges, buildings, transmission towers, construction equipment, offshore structures, and structural members.
Key Differences
EN 10025-3 S460N specifies Ni, N, Al, Ti which are not specified for ASTM A572 Gr.65.
Can EN 10025-3 S460N Be Substituted With ASTM A572 Gr.65?
EN 10025-3 S460N and ASTM A572 Gr.65 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10025-3 S460N and ASTM A572 Gr.65?
EN 10025-3 S460N specifies Ni, N, Al, Ti which are not specified for ASTM A572 Gr.65.