Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
EN 10025-5 S420J2W (EN 10025-5:2019) and CSA G40.21 50W (CSA G40.21-13 (R2023)) are both steel grades.
Both fall under the Structural Steel (Corten / Weathering) category.
EN 10025-5 S420J2W is defined under European Standard (EN), originating from Europe, while CSA G40.21 50W is defined under Canadian Standards Association (CSA), originating from Canada.
As per chemical composition, EN 10025-5 S420J2W vs CSA G40.21 50W is a 80.4% match.
As per mechanical properties, the match is 57.9%.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10025-5 S420J2W
CSA G40.21 50W
Tensile Strength
500-660 MPa
450-655 MPa (65-95 ksi)
Yield Strength
>=420 MPa
345 MPa (50 ksi) min
Elongation
>=19%
19% min
Condition
Nominal thickness up to 16 mm for yield, 3 to 100 mm for tensile, 3 to 40 mm for elongation (Lo = 5.65 sqrt(S0), longitudinal); transverse values are lower, see blocks
EN 10025-5 S420J2W specifies N which is not specified for CSA G40.21 50W.
CSA G40.21 50W specifies Ni which is not specified for EN 10025-5 S420J2W.
Can EN 10025-5 S420J2W Be Substituted With CSA G40.21 50W?
EN 10025-5 S420J2W and CSA G40.21 50W share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10025-5 S420J2W and CSA G40.21 50W?
EN 10025-5 S420J2W specifies N which is not specified for CSA G40.21 50W. CSA G40.21 50W specifies Ni which is not specified for EN 10025-5 S420J2W.
Can EN 10025-5 S420J2W be substituted with CSA G40.21 50W?
EN 10025-5 S420J2W and CSA G40.21 50W share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.