EN 10028-2 P235GH vs EN 10025-3 S275NL

Related Material — 65% match based on chemical composition and mechanical property overlap.

EN 10028-2 P235GH (EN 10028-2:2017) and EN 10025-3 S275NL (EN 10025-3:2019) are both steel grades. EN 10028-2 P235GH is classified under Carbon Steel, while EN 10025-3 S275NL is classified under Structural Steel — a different category, which is worth noting alongside the chemistry match below. EN 10028-2 P235GH is defined under European Standard (EN), originating from Europe, while EN 10025-3 S275NL is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10028-2 P235GH vs EN 10025-3 S275NL is a 84% match. As per mechanical properties, the match is 57.8%. Combined, this makes them a related material overall at 65%.

Frequently Compared With EN 10028-2 P235GH:
BS 970 (Part 1) 060A32 BS 970 (Part 1) 045A10 BS 970 (Part 1) 045M10 BS 970 (Part 1) 045A10 BS 970 (Part 3) 045A10 BS 970 (Part 1) 040A04 BS 970 (Part 1) 040A12 BS 970 (Part 1) 045M10 BS 970 (Part 3) 045M10 BS 970 (Part 1) 040A10 BS 970 (Part 1) 055M15 BS 970 (Part 1) 060A40
Match Breakdown
CHEMISTRY MATCH
84%
MECHANICAL MATCH
57.8%
OVERALL
65%
Specifications
Property EN 10028-2 P235GH EN 10025-3 S275NL
Standard EN 10028-2:2017 EN 10025-3:2019
Category Carbon Steel Structural Steel
C (%) <=0.16 <=0.16
Si (%) <=0.35 <=0.40
Mn (%) 0.60-1.20 0.50-1.50
P (%) <=0.025 <=0.025
S (%) <=0.010 <=0.020
Nb (%) <=0.030 <=0.05
Al (%) >=0.020 >=0.02
N (%) <=0.012 <=0.015
Cr (%) <=0.30 <=0.30
Cu (%) <=0.30 <=0.55
Mo (%) <=0.08 <=0.10
Ni (%) <=0.30 <=0.30
Ti (%) <=0.03 <=0.05
V (%) <=0.02 <=0.05
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10028-2 P235GH EN 10025-3 S275NL
Tensile Strength 360-480 MPa 370-510 MPa
Yield Strength >=235 MPa >=275 MPa
Elongation >=24% >=24%
Condition Usual delivery condition normalized (+N), nominal thickness up to 16 mm; transverse direction, Yield Strength is ReH, Elongation is A Normalized or normalized rolled (N), nominal thickness up to 16 mm (tensile strength up to 100 mm), Table 4
Typical Applications
EN 10028-2 P235GH
Flat products for pressure purposes
EN 10025-3 S275NL
Not documented
Key Differences
Can EN 10028-2 P235GH Be Substituted With EN 10025-3 S275NL?
EN 10028-2 P235GH and EN 10025-3 S275NL share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
EN 10028-2 P235GH
0 active listings and RFQs →
EN 10025-3 S275NL
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10028-2 P235GH and EN 10025-3 S275NL?
Different category: EN 10028-2 P235GH is Carbon Steel, EN 10025-3 S275NL is Structural Steel.
Can EN 10028-2 P235GH be substituted with EN 10025-3 S275NL?
EN 10028-2 P235GH and EN 10025-3 S275NL share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.