Minimal Match — 30.5% match
based on chemical composition and mechanical property overlap.
EN 10028-3 P460NH (EN 10028-3:2017) and UNI 11234 100Cr6 (UNI 11234:2007) are both steel grades.
Both fall under the Alloy Steel category.
EN 10028-3 P460NH is typically used for flat products for pressure equipment, while UNI 11234 100Cr6 is commonly used for ball bearings,roller bearings,needle bearings,dies,punches,gauges,wear resistant components.
EN 10028-3 P460NH is defined under European Standard (EN), originating from Europe, while UNI 11234 100Cr6 is defined under Ente Nazionale Italiano di Unificazione (UNI), originating from Italy.
As per chemical composition, EN 10028-3 P460NH vs UNI 11234 100Cr6 is a 45.8% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a minimal match overall at 30.5%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
EN 10028-3 P460NH specifies Al, N, Cu, Mo which are not specified for UNI 11234 100Cr6.
Can EN 10028-3 P460NH Be Substituted With UNI 11234 100Cr6?
EN 10028-3 P460NH and UNI 11234 100Cr6 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10028-3 P460NH and UNI 11234 100Cr6?
EN 10028-3 P460NH specifies Al, N, Cu, Mo which are not specified for UNI 11234 100Cr6.
Can EN 10028-3 P460NH be substituted with UNI 11234 100Cr6?
EN 10028-3 P460NH and UNI 11234 100Cr6 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.