EN 10088-1 1.4401 vs ASTM A959 201L

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4401 (EN 10088-1:2014) and ASTM A959 201L (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4401 is typically used for marine, chemical processing, pharmaceutical equipment, while ASTM A959 201L is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1). EN 10088-1 1.4401 is defined under European Standard (EN), originating from Europe, while ASTM A959 201L is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 1.4401 vs ASTM A959 201L is a 60% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 1.4401:
EN 10088-1 1.4845 EN 10088-1 1.4301 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 GOST 5632 12Kh13 GOST 5632 06Kh23N28 EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 20Cr12MoNiVH IS 1570 (Part 7) 12Cr12MoH
Match Breakdown
CHEMISTRY MATCH
60%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property EN 10088-1 1.4401 ASTM A959 201L
Standard EN 10088-1:2014 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) ≤0.07 <=0.03
Si (%) ≤1.00 <=1.00
Mn (%) ≤2.00 5.5-7.5
Cr (%) 16.5–18.5 16.0-18.0
Ni (%) 10.5–13.5 3.5-5.5
Mo (%) 2.0–2.5 Not specified
N (%) Not specified <=0.25
P (%) Not specified <=0.045
S (%) Not specified <=0.030
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4401 ASTM A959 201L
Tensile Strength ≥520 MPa Not specified
Yield Strength ≥210 MPa Not specified
Elongation ≥40% Not specified
Hardness ≤215 HB Not specified
Typical Applications
EN 10088-1 1.4401
Marine, chemical processing, pharmaceutical equipment
ASTM A959 201L
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
Can EN 10088-1 1.4401 Be Substituted With ASTM A959 201L?
EN 10088-1 1.4401 and ASTM A959 201L share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 1.4401
Sheet → (4 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3400 mm (98.43–133.86 in)
ASTM A959 201L
No active listings currently.
On M-EX Right Now
EN 10088-1 1.4401
4 active listings and RFQs →
ASTM A959 201L
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4401 and ASTM A959 201L?
EN 10088-1 1.4401 specifies Mo which is not specified for ASTM A959 201L. ASTM A959 201L specifies N, P, S which are not specified for EN 10088-1 1.4401.
Can EN 10088-1 1.4401 be substituted with ASTM A959 201L?
EN 10088-1 1.4401 and ASTM A959 201L share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.