EN 10088-1 X10CrMoVNb9-1 vs IS 4367 10Cr9Mo10

Related Material — 59.3% match based on chemical composition and mechanical property overlap.

EN 10088-1 X10CrMoVNb9-1 (EN 10088-1:2014) and IS 4367 10Cr9Mo10 (IS 4367:1991) are both steel grades. EN 10088-1 X10CrMoVNb9-1 is classified under Stainless Steel, while IS 4367 10Cr9Mo10 is classified under Alloy Steel — a different category, which is worth noting alongside the chemistry match below. EN 10088-1 X10CrMoVNb9-1 is defined under European Standard (EN), originating from Europe, while IS 4367 10Cr9Mo10 is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, EN 10088-1 X10CrMoVNb9-1 vs IS 4367 10Cr9Mo10 is a 59.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 59.3%.

Frequently Compared With EN 10088-1 X10CrMoVNb9-1:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
59.3%
MECHANICAL MATCH
No shared data
OVERALL
59.3%
Specifications
Property EN 10088-1 X10CrMoVNb9-1 IS 4367 10Cr9Mo10
Standard EN 10088-1:2014 IS 4367:1991
Category Stainless Steel Alloy Steel
C (%) 0.08-0.12 <=0.15
Si (%) <=0.50 <=0.50
Mn (%) 0.30-0.60 0.40-0.70
P (%) <=0.025 <=0.035
S (%) <=0.015 <=0.035
Cr (%) 8.0-9.5 2.00-2.50
Mo (%) 0.85-1.05 0.90-1.10
Ni (%) <=0.40 <=0.30
N (%) 0.030-0.070 Not specified
Al (%) <=0.040 Not specified
Nb (%) 0.060-0.10 Not specified
V (%) 0.18-0.25 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X10CrMoVNb9-1 IS 4367 10Cr9Mo10
Tensile Strength Not specified 410-590 MPa
Yield Strength Not specified 245 MPa min
Elongation Not specified >=18%
Izod Impact Not specified 55 J min
Hardness (soft annealed) Not specified <=187 HB
Condition Not specified Normalised and tempered, ruling section up to 50 mm
Key Differences
Can EN 10088-1 X10CrMoVNb9-1 Be Substituted With IS 4367 10Cr9Mo10?
EN 10088-1 X10CrMoVNb9-1 and IS 4367 10Cr9Mo10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
EN 10088-1 X10CrMoVNb9-1
0 active listings and RFQs →
IS 4367 10Cr9Mo10
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X10CrMoVNb9-1 and IS 4367 10Cr9Mo10?
Different category: EN 10088-1 X10CrMoVNb9-1 is Stainless Steel, IS 4367 10Cr9Mo10 is Alloy Steel. EN 10088-1 X10CrMoVNb9-1 specifies N, Al, Nb, V which are not specified for IS 4367 10Cr9Mo10.
Can EN 10088-1 X10CrMoVNb9-1 be substituted with IS 4367 10Cr9Mo10?
EN 10088-1 X10CrMoVNb9-1 and IS 4367 10Cr9Mo10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.