EN 10088-1 X12CrNiWTiB16-13 vs GOST 5632 06Kh23N28

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 X12CrNiWTiB16-13 (EN 10088-1:2014) and GOST 5632 06Kh23N28 (GOST 5632-2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X12CrNiWTiB16-13 is defined under European Standard (EN) (Europe).

As per chemical composition, EN 10088-1 X12CrNiWTiB16-13 vs GOST 5632 06Kh23N28 is a 45.7% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 X12CrNiWTiB16-13:
IS 1570 (Part 7) 11Cr17Ni13W3TiH EN 10088-1 1.4006 EN 10088-1 1.4301 ASTM A959 .- EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
45.7%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property EN 10088-1 X12CrNiWTiB16-13 GOST 5632 06Kh23N28
Standard EN 10088-1:2014 GOST 5632-2014
Category Stainless Steel Stainless Steel
C (%) 0.07-0.15 ≤0.06
Si (%) <=0.50 ≤0.80
Mn (%) <=1.50 ≤2.00
P (%) <=0.035 Not specified
S (%) <=0.015 Not specified
Cr (%) 15.5-17.5 22.0–25.0
Ni (%) 12.5-14.5 26.0–29.0
Ti (%) 0.40-0.70 Not specified
W (%) 2.50-3.00 Not specified
B (%) 0.0015-0.0060 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X12CrNiWTiB16-13 GOST 5632 06Kh23N28
Tensile Strength Not specified ≥510 MPa
Yield Strength Not specified ≥196 MPa
Elongation Not specified ≥35%
Max Service Temp Not specified 1050°C
Typical Applications
EN 10088-1 X12CrNiWTiB16-13
Not documented
GOST 5632 06Kh23N28
Furnace components, heat exchangers, high temperature applications
Key Differences
Can EN 10088-1 X12CrNiWTiB16-13 Be Substituted With GOST 5632 06Kh23N28?
EN 10088-1 X12CrNiWTiB16-13 and GOST 5632 06Kh23N28 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 X12CrNiWTiB16-13
No active listings currently.
GOST 5632 06Kh23N28
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 3100–3400 mm (122.05–133.86 in)
On M-EX Right Now
EN 10088-1 X12CrNiWTiB16-13
0 active listings and RFQs →
GOST 5632 06Kh23N28
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X12CrNiWTiB16-13 and GOST 5632 06Kh23N28?
EN 10088-1 X12CrNiWTiB16-13 specifies P, S, Ti, W which are not specified for GOST 5632 06Kh23N28.
Can EN 10088-1 X12CrNiWTiB16-13 be substituted with GOST 5632 06Kh23N28?
EN 10088-1 X12CrNiWTiB16-13 and GOST 5632 06Kh23N28 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.