EN 10088-1 X12NiCrSi35-16 vs EN 10088-1 1.4301

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 X12NiCrSi35-16 (EN 10088-1:2014) and EN 10088-1 1.4301 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X12NiCrSi35-16 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4301 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X12NiCrSi35-16 vs EN 10088-1 1.4301 is a 61.8% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 X12NiCrSi35-16:
EN 10088-1 1.4845 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
61.8%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property EN 10088-1 X12NiCrSi35-16 EN 10088-1 1.4301
Standard EN 10088-1:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.15 ≤0.07
Si (%) 1.00-2.00 ≤1.00
Mn (%) <=2.00 ≤2.00
P (%) <=0.045 ≤0.045
S (%) <=0.015 ≤0.030
Cr (%) 15.0-17.0 17.5–19.5
Ni (%) 33.0-37.0 8.0–10.5
N (%) <=0.10 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X12NiCrSi35-16 EN 10088-1 1.4301
Tensile Strength Not specified ≥520 MPa
Yield Strength Not specified ≥210 MPa
Elongation Not specified ≥45%
Hardness Not specified ≤215 HB
Typical Applications
EN 10088-1 X12NiCrSi35-16
Not documented
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
Key Differences
Can EN 10088-1 X12NiCrSi35-16 Be Substituted With EN 10088-1 1.4301?
EN 10088-1 X12NiCrSi35-16 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 X12NiCrSi35-16
No active listings currently.
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
On M-EX Right Now
EN 10088-1 X12NiCrSi35-16
0 active listings and RFQs →
EN 10088-1 1.4301
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X12NiCrSi35-16 and EN 10088-1 1.4301?
EN 10088-1 X12NiCrSi35-16 specifies N which is not specified for EN 10088-1 1.4301.
Can EN 10088-1 X12NiCrSi35-16 be substituted with EN 10088-1 1.4301?
EN 10088-1 X12NiCrSi35-16 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.