EN 10088-1 X17CrNi16-2 vs IS 6911 X15Cr16Ni2

Strong Match — 92% match based on chemical composition and mechanical property overlap.

EN 10088-1 X17CrNi16-2 (EN 10088-1:2014) and IS 6911 X15Cr16Ni2 (IS 6911:1992) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X17CrNi16-2 is defined under European Standard (EN), originating from Europe, while IS 6911 X15Cr16Ni2 is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, EN 10088-1 X17CrNi16-2 vs IS 6911 X15Cr16Ni2 is a 92% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 92%.

Frequently Compared With EN 10088-1 X17CrNi16-2:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
92%
MECHANICAL MATCH
No shared data
OVERALL
92%
Specifications
Property EN 10088-1 X17CrNi16-2 IS 6911 X15Cr16Ni2
Standard EN 10088-1:2014 IS 6911:1992
Category Stainless Steel Stainless Steel
C (%) 0.12-0.22 0.10-0.20
Si (%) <=1.00 <=1.0
Mn (%) <=1.50 <=1.0
P (%) <=0.040 <=0.045
S (%) <=0.015 <=0.030
Cr (%) 15.0-17.0 15.0-17.0
Ni (%) 1.50-2.50 1.25-2.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X17CrNi16-2 IS 6911 X15Cr16Ni2
Elongation (50 mm, annealed) Not specified >=10%
Hardness (annealed, max) Not specified 262 HBS
Tensile Strength (annealed) Not specified >=830 MPa
Yield Strength (0.2% proof, annealed) Not specified >=640 MPa
Typical Applications
EN 10088-1 X17CrNi16-2
Not documented
IS 6911 X15Cr16Ni2
Stainless and heat-resisting steel plate, sheet and strip (clause 1.1)
Can EN 10088-1 X17CrNi16-2 Be Substituted With IS 6911 X15Cr16Ni2?
EN 10088-1 X17CrNi16-2 and IS 6911 X15Cr16Ni2 overlap closely enough on chemistry and mechanical properties that IS 6911 X15Cr16Ni2 is often considered as a substitute for EN 10088-1 X17CrNi16-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X17CrNi16-2
0 active listings and RFQs →
IS 6911 X15Cr16Ni2
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X17CrNi16-2 and IS 6911 X15Cr16Ni2?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X17CrNi16-2 be substituted with IS 6911 X15Cr16Ni2?
EN 10088-1 X17CrNi16-2 and IS 6911 X15Cr16Ni2 overlap closely enough on chemistry and mechanical properties that IS 6911 X15Cr16Ni2 is often considered as a substitute for EN 10088-1 X17CrNi16-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.