EN 10088-1 X1CrNiMoCuN25-25-5 vs ASTM A240/A240M N08932

Strong Match — 89.1% match based on chemical composition and mechanical property overlap.

EN 10088-1 X1CrNiMoCuN25-25-5 (EN 10088-1:2014) and ASTM A240/A240M N08932 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X1CrNiMoCuN25-25-5 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M N08932 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X1CrNiMoCuN25-25-5 vs ASTM A240/A240M N08932 is a 89.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 89.1%.

Frequently Compared With EN 10088-1 X1CrNiMoCuN25-25-5:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
89.1%
MECHANICAL MATCH
No shared data
OVERALL
89.1%
Specifications
Property EN 10088-1 X1CrNiMoCuN25-25-5 ASTM A240/A240M N08932
Standard EN 10088-1:2014 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Si (%) <=0.70 <=0.40
Mn (%) <=2.00 <=2.00
P (%) <=0.030 <=0.025
S (%) <=0.010 <=0.010
Cr (%) 24.0-26.0 24.0-26.0
Mo (%) 4.7-5.7 4.5-6.5
Ni (%) 24.0-27.0 24.0-26.0
N (%) 0.17-0.25 0.15-0.25
Cu (%) 1.00-2.00 1.0-2.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X1CrNiMoCuN25-25-5 ASTM A240/A240M N08932
Tensile Strength Not specified >=600 MPa
Yield Strength Not specified >=305 MPa
Elongation Not specified >=40%
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
EN 10088-1 X1CrNiMoCuN25-25-5
Not documented
ASTM A240/A240M N08932
Pressure vessels and general applications (plate, sheet and strip)
Can EN 10088-1 X1CrNiMoCuN25-25-5 Be Substituted With ASTM A240/A240M N08932?
EN 10088-1 X1CrNiMoCuN25-25-5 and ASTM A240/A240M N08932 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08932 is often considered as a substitute for EN 10088-1 X1CrNiMoCuN25-25-5 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X1CrNiMoCuN25-25-5
0 active listings and RFQs →
ASTM A240/A240M N08932
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X1CrNiMoCuN25-25-5 and ASTM A240/A240M N08932?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X1CrNiMoCuN25-25-5 be substituted with ASTM A240/A240M N08932?
EN 10088-1 X1CrNiMoCuN25-25-5 and ASTM A240/A240M N08932 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08932 is often considered as a substitute for EN 10088-1 X1CrNiMoCuN25-25-5 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.