EN 10088-1 X2CrMoTi18-2 vs EN 10088-2 X2CrMoTi18-2

Strong Match — 94.8% match based on chemical composition and mechanical property overlap.

EN 10088-1 X2CrMoTi18-2 (EN 10088-1:2014) and EN 10088-2 X2CrMoTi18-2 (EN 10088-2:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X2CrMoTi18-2 is defined under European Standard (EN), originating from Europe, while EN 10088-2 X2CrMoTi18-2 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X2CrMoTi18-2 vs EN 10088-2 X2CrMoTi18-2 is a 94.8% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 94.8%.

Frequently Compared With EN 10088-1 X2CrMoTi18-2:
ASTM A959 .- GOST 5632 08X18H10 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr13H GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
94.8%
MECHANICAL MATCH
No shared data
OVERALL
94.8%
Specifications
Property EN 10088-1 X2CrMoTi18-2 EN 10088-2 X2CrMoTi18-2
Standard EN 10088-1:2014 EN 10088-2:2014
Category Stainless Steel Stainless Steel
C (%) <=0.025 <=0.025
Si (%) <=1.00 <=1.00
Mn (%) <=1.00 <=1.00
P (%) <=0.040 <=0.040
S (%) <=0.015 <=0.015
Cr (%) 17.0-20.0 17.0-20.0
Mo (%) 1.80-2.50 1.80-2.50
N (%) <=0.030 <=0.030
Ti (%) Not specified <=0.80
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X2CrMoTi18-2 EN 10088-2 X2CrMoTi18-2
Tensile Strength Not specified 420-640 MPa
Condition Not specified Annealed (+A), cold rolled strip, up to 8 mm thick; Elongation is A80 (under 3 mm) or A (3 mm and over), longitudinal and transverse
Yield Strength Not specified >=300 MPa
Elongation Not specified >=20%
Typical Applications
EN 10088-1 X2CrMoTi18-2
Not documented
EN 10088-2 X2CrMoTi18-2
General purposes, hot or cold rolled sheet/plate and strip
Key Differences
Can EN 10088-1 X2CrMoTi18-2 Be Substituted With EN 10088-2 X2CrMoTi18-2?
EN 10088-1 X2CrMoTi18-2 and EN 10088-2 X2CrMoTi18-2 overlap closely enough on chemistry and mechanical properties that EN 10088-2 X2CrMoTi18-2 is often considered as a substitute for EN 10088-1 X2CrMoTi18-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X2CrMoTi18-2
0 active listings and RFQs →
EN 10088-2 X2CrMoTi18-2
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X2CrMoTi18-2 and EN 10088-2 X2CrMoTi18-2?
EN 10088-2 X2CrMoTi18-2 specifies Ti which is not specified for EN 10088-1 X2CrMoTi18-2.
Can EN 10088-1 X2CrMoTi18-2 be substituted with EN 10088-2 X2CrMoTi18-2?
EN 10088-1 X2CrMoTi18-2 and EN 10088-2 X2CrMoTi18-2 overlap closely enough on chemistry and mechanical properties that EN 10088-2 X2CrMoTi18-2 is often considered as a substitute for EN 10088-1 X2CrMoTi18-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.