EN 10088-1 X2CrNiMnMoCuN24-4-3-2 vs EN 10088-1 1.4401

Minimal Match — 49.3% match based on chemical composition and mechanical property overlap.

EN 10088-1 X2CrNiMnMoCuN24-4-3-2 (EN 10088-1:2014) and EN 10088-1 1.4401 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X2CrNiMnMoCuN24-4-3-2 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4401 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X2CrNiMnMoCuN24-4-3-2 vs EN 10088-1 1.4401 is a 49.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 49.3%.

Frequently Compared With EN 10088-1 X2CrNiMnMoCuN24-4-3-2:
GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
49.3%
MECHANICAL MATCH
No shared data
OVERALL
49.3%
Specifications
Property EN 10088-1 X2CrNiMnMoCuN24-4-3-2 EN 10088-1 1.4401
Standard EN 10088-1:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.030 ≤0.07
Si (%) <=0.70 ≤1.00
Mn (%) 2.50-4.0 ≤2.00
P (%) <=0.035 Not specified
S (%) <=0.005 Not specified
Cr (%) 23.0-25.0 16.5–18.5
Mo (%) 1.00-2.00 2.0–2.5
Ni (%) 3.0-4.5 10.5–13.5
N (%) 0.20-0.30 Not specified
Cu (%) 0.10-0.80 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X2CrNiMnMoCuN24-4-3-2 EN 10088-1 1.4401
Tensile Strength Not specified ≥520 MPa
Yield Strength Not specified ≥210 MPa
Elongation Not specified ≥40%
Hardness Not specified ≤215 HB
Typical Applications
EN 10088-1 X2CrNiMnMoCuN24-4-3-2
Not documented
EN 10088-1 1.4401
Marine, chemical processing, pharmaceutical equipment
Key Differences
Can EN 10088-1 X2CrNiMnMoCuN24-4-3-2 Be Substituted With EN 10088-1 1.4401?
EN 10088-1 X2CrNiMnMoCuN24-4-3-2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 X2CrNiMnMoCuN24-4-3-2
No active listings currently.
EN 10088-1 1.4401
Sheet → (4 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3400 mm (98.43–133.86 in)
On M-EX Right Now
EN 10088-1 X2CrNiMnMoCuN24-4-3-2
0 active listings and RFQs →
EN 10088-1 1.4401
4 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X2CrNiMnMoCuN24-4-3-2 and EN 10088-1 1.4401?
EN 10088-1 X2CrNiMnMoCuN24-4-3-2 specifies P, S, N, Cu which are not specified for EN 10088-1 1.4401.
Can EN 10088-1 X2CrNiMnMoCuN24-4-3-2 be substituted with EN 10088-1 1.4401?
EN 10088-1 X2CrNiMnMoCuN24-4-3-2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.