EN 10088-1 X6CrNi23-13 vs ASTM A240/A240M S30909

Strong Match — 92.1% match based on chemical composition and mechanical property overlap.

EN 10088-1 X6CrNi23-13 (EN 10088-1:2014) and ASTM A240/A240M S30909 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X6CrNi23-13 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M S30909 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X6CrNi23-13 vs ASTM A240/A240M S30909 is a 92.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 92.1%.

Frequently Compared With EN 10088-1 X6CrNi23-13:
GOST 5632 08X18H10 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr13H ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
92.1%
MECHANICAL MATCH
No shared data
OVERALL
92.1%
Specifications
Property EN 10088-1 X6CrNi23-13 ASTM A240/A240M S30909
Standard EN 10088-1:2014 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) 0.04-0.08 0.04-0.10
Si (%) <=0.70 <=0.75
Mn (%) <=2.00 <=2.00
P (%) <=0.035 <=0.045
S (%) <=0.015 <=0.030
Cr (%) 22.0-24.0 22.0-24.0
Ni (%) 12.0-15.0 12.0-15.0
N (%) <=0.10 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X6CrNi23-13 ASTM A240/A240M S30909
Tensile Strength Not specified >=515 MPa
Yield Strength Not specified >=205 MPa
Elongation Not specified >=40%
Hardness Not specified <=217 HB
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
EN 10088-1 X6CrNi23-13
Not documented
ASTM A240/A240M S30909
Pressure vessels and general applications (plate, sheet and strip)
Key Differences
Can EN 10088-1 X6CrNi23-13 Be Substituted With ASTM A240/A240M S30909?
EN 10088-1 X6CrNi23-13 and ASTM A240/A240M S30909 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S30909 is often considered as a substitute for EN 10088-1 X6CrNi23-13 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X6CrNi23-13
0 active listings and RFQs →
ASTM A240/A240M S30909
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X6CrNi23-13 and ASTM A240/A240M S30909?
EN 10088-1 X6CrNi23-13 specifies N which is not specified for ASTM A240/A240M S30909.
Can EN 10088-1 X6CrNi23-13 be substituted with ASTM A240/A240M S30909?
EN 10088-1 X6CrNi23-13 and ASTM A240/A240M S30909 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M S30909 is often considered as a substitute for EN 10088-1 X6CrNi23-13 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.