EN 10088-1 X10NiCrAlTi32-21 vs ASTM A959 N08811

Strong Match — 88.1% match based on chemical composition and mechanical property overlap.

EN 10088-1 X10NiCrAlTi32-21 (EN 10088-1:2023) and ASTM A959 N08811 (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X10NiCrAlTi32-21 is defined under European Standard (EN), originating from Europe, while ASTM A959 N08811 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X10NiCrAlTi32-21 vs ASTM A959 N08811 is a 88.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 88.1%.

Frequently Compared With EN 10088-1 X10NiCrAlTi32-21:
ASTM A959 .- GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4301 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
88.1%
MECHANICAL MATCH
No shared data
OVERALL
88.1%
Specifications
Property EN 10088-1 X10NiCrAlTi32-21 ASTM A959 N08811
Standard EN 10088-1:2023 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.12 0.06-0.10
Si (%) <=1.00 <=1.00
Mn (%) <=2.00 <=1.50
P (%) <=0.030 <=0.040
S (%) <=0.015 <=0.015
Cr (%) 19.0-23.0 19.0-23.0
Ni (%) 30.0-34.0 30.0-35.0
Al (%) 0.15-0.60 0.15-0.60
Ti (%) 0.15-0.60 0.15-0.60
Cu (%) Not specified <=0.75
Fe (%) Not specified >=39.5
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
EN 10088-1 X10NiCrAlTi32-21
Not documented
ASTM A959 N08811
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
Can EN 10088-1 X10NiCrAlTi32-21 Be Substituted With ASTM A959 N08811?
EN 10088-1 X10NiCrAlTi32-21 and ASTM A959 N08811 overlap closely enough on chemistry and mechanical properties that ASTM A959 N08811 is often considered as a substitute for EN 10088-1 X10NiCrAlTi32-21 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X10NiCrAlTi32-21
0 active listings and RFQs →
ASTM A959 N08811
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X10NiCrAlTi32-21 and ASTM A959 N08811?
ASTM A959 N08811 specifies Cu, Fe which are not specified for EN 10088-1 X10NiCrAlTi32-21.
Can EN 10088-1 X10NiCrAlTi32-21 be substituted with ASTM A959 N08811?
EN 10088-1 X10NiCrAlTi32-21 and ASTM A959 N08811 overlap closely enough on chemistry and mechanical properties that ASTM A959 N08811 is often considered as a substitute for EN 10088-1 X10NiCrAlTi32-21 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.