EN 10088-1 X12CrCoNi21-20 vs EN 10088-1 X12CrCoNi21-20

Strong Match — 100% match based on chemical composition and mechanical property overlap.

EN 10088-1 X12CrCoNi21-20 (EN 10088-1:2023) and EN 10088-1 X12CrCoNi21-20 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X12CrCoNi21-20 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X12CrCoNi21-20 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X12CrCoNi21-20 vs EN 10088-1 X12CrCoNi21-20 is a 100% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 100%.

Frequently Compared With EN 10088-1 X12CrCoNi21-20:
EN 10088-1 1.4845 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- GB/T 3280 06Cr19Ni10
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
No shared data
OVERALL
100%
Specifications
Property EN 10088-1 X12CrCoNi21-20 EN 10088-1 X12CrCoNi21-20
Standard EN 10088-1:2023 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.08-0.16 0.08-0.16
Si (%) <=1.00 <=1.00
Mn (%) <=2.00 <=2.00
P (%) <=0.035 <=0.035
S (%) <=0.015 <=0.015
Cr (%) 20.0-22.5 20.0-22.5
Mo (%) 2.50-3.5 2.50-3.5
Ni (%) 19.0-21.0 19.0-21.0
N (%) 0.10-0.20 0.10-0.20
Nb (%) 0.75-1.25 0.75-1.25
W (%) 2.00-3.00 2.00-3.00
Co (%) 18.5-21.0 18.5-21.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Can EN 10088-1 X12CrCoNi21-20 Be Substituted With EN 10088-1 X12CrCoNi21-20?
EN 10088-1 X12CrCoNi21-20 and EN 10088-1 X12CrCoNi21-20 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X12CrCoNi21-20 is often considered as a substitute for EN 10088-1 X12CrCoNi21-20 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X12CrCoNi21-20
0 active listings and RFQs →
EN 10088-1 X12CrCoNi21-20
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X12CrCoNi21-20 and EN 10088-1 X12CrCoNi21-20?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X12CrCoNi21-20 be substituted with EN 10088-1 X12CrCoNi21-20?
EN 10088-1 X12CrCoNi21-20 and EN 10088-1 X12CrCoNi21-20 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X12CrCoNi21-20 is often considered as a substitute for EN 10088-1 X12CrCoNi21-20 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.